30 Terms

1
New cards

What is Corrosion?

Degradation of metals due to chemical or electrochemical reactions

2
New cards

Dry desert climates

Which environment is particularly detrimental to aircraft?

3
New cards

Reddish rust

What is a common sign of corrosion on steel?

4
New cards

Pilot age

Which factor does NOT affect corrosion?

5
New cards

High corrosion – resistant

Pure metals are generally:

6
New cards

Magnesium and aluminum

Which metals corrode easily?

7
New cards

Is more harmful to aircraft

In marine environments, moisture – laden air:

8
New cards

High humidity

Which factor increases corrosion rate?

9
New cards

Accelerate corrosion

Foreign material such as oil and dust can:

10
New cards

Increase dampness and corrosion

Micro – organisms on surfaces can:

11
New cards

Caustic liquid or gaseous agents

Direct chemical attack occurs due to:

12
New cards

Sealed lead – acid

Which battery type reduces acid spillage issues?

13
New cards

Four specific conditions

Electrochemical corrosion requires:

14
New cards

Wormlike traces

Surface corrosion is recognized by:

15
New cards

Wormlike traces under paint

Filiform corrosion appears as:

16
New cards

Aluminum and magnesium alloys

Pitting corrosion is common in:

17
New cards

Contact with dissimilar metals and electrolyte

Dissimilar metal corrosion can occur due to:

18
New cards

Crevice corrosion

Concentration cell corrosion is also called:

19
New cards

Grain boundaries of alloys

Intergranular corrosion attacks:

20
New cards

Intergranular corrosion

Exfoliation corrosion is an advanced form of:

21
New cards

Cannot always be detected by surface indications

Intergranular corrosion in aluminum alloy parts

22
New cards

The surface area of the anodic metal is smaller than the surface area of the cathodic metal

Galvanic corrosion is likely to be most rapid and severe when

23
New cards

Only when two dissimilar metals are in contact

Fretting corrosion is most likely to occur

24
New cards

Magnesium

Which of these materials is the most anodic?

25
New cards

Exfoliation

The lifting or flaking of the metal at the surface due to delamination of grain boundaries caused by the pressure of corrosion residual product buildup is called

26
New cards

Corrosion

Caustic cleaning products used on aluminum structures have the effect of producing

27
New cards

The presence of a passive oxide film

Which of the listed conditions is NOT one of the requirements for corrosion to occur?

28
New cards

Stainless steel

Which of these materials is the most cathodic?

29
New cards

Improper heat treatment

A primary cause of intergranular corrosion is

30
New cards

Intergranular corrosion

Which of the following may not be detectable even by careful visual inspection of the surface of aluminum alloy parts of structures?