1/16
Looks like no tags are added yet.
Fluid state
“workability” or ease/flow of the concrete
measured by slump test
Bleeding
when water rises to surface of fresh poured concrete and brings small particles of cement
too much bleeding can cause poor bonding between cement paste and aggregate
Settlement
when heavier solid materials in fresh concrete sink downward, causes concrete to compact and water to rise to surface
Segregation
aggregate is separated from the cement paste matrix
Consolidation
removing trapped air from freshly placed concrete by vibrating/compacting to make concrete denser/stronger
too low of a slump can lead to poor consolidation unless properly placed
Setting
solidifying concrete
“initial set”: fluid to solid
“final set”: starts to gain strength
Mixture proportions (compressive strength)
amount of each ingredient used in concrete
age (compressive strength)
longer concrete cures, stronger becomes
7 day strength is 75% of 28 day
uniformity (compressive strength)
how evenly the materials are mixed and distributed
degree of consolidation (compressive strength)
how well air bubbles are removed from concrete, better consolidation stronger concrete
nature of load (compressive strength)
the type of force of pressure placed on concrete
pre-life
planning the concrete recipe based on materials available
mix
combine cement water sand and gravel
placeability
how easily concrete can be poured and put into position
consolidation property
removing trapped air from concrete to make it denser
finishing property
smoothing and shaping concrete surface
water to cement ratio
amount of water compared to cement
compressive strength is inversely related
lower w/c = stronger concrete
higher w/c = weaker concrete