1/177
Looks like no tags are added yet.
Cold Work
O, W, A, D
O series (Cold Work)
Oil Hardening
O1, O2, O6, O7
W series (Cold Work)
Water Hardening
W1, W2, W5
A series (Cold Work)
Medium Alloy Air Hardening
A2, A4, A6, A8, A9, A10, A11
D series (Cold Work)
High Carbon, High Chromium
D2, D3, D4, D5, D7
Shock Resisting
S series
S1, S2, S4, S5, S6, S7
Hot Work
H, P
H Series (Hot Work)
H10-H19 Chromium Types
H20-H39 Tungsten Types
H40-H59 Molybdenum Types
P series (Hot Work)
Molded
P6, P20, P21
High Speed
M, T
M series (High Speed)
Molybdenum Types
M1, M2, M3-1, M3-2, M4, M6, M7, M10, M33, M36, M41, M46, M50
T series (High Speed)
Tungsten Types
T1, T4, T5, T6, T8, T15
Special Purpose
L series
L2, L6
Carbon steel Hardening Properties
Hardenability: Biggest back curve/worst hardenability
Hardness: Sharp drop as Temper Temp Increases
Abrasion Resistance: Wear volume grows the most over time
Alloy Steel Hardening Properties
Hardenability: Middle Largest Back curve/middle hardenability
Hardness: Slow decline
Abrasion Resistance: Medium wear volume amount
Tool Steels
Hardenability: Smallest Back curve/best hardenability
Hardness: Goes down a little, then back up, then sharp drop
Abrasion Resistance: Least amount of wear volume
Safety in Hardening
Risk of Damaging from hardneing (quench cracks)
Eutectic Structures
spread out carbide structures
Eutectic Networks
Long multiple chains of carbide structures
Severe Banding (cause and effect)
-caused by segregation of the alloying elements during solidification
-causes anisotropy in the tensile ductility and impact energy of the steels
Why are eutectic material and severe banding undesirable?
Makes the tool steel crack easier
Hardening Characteristics (4)
Safety in Hardening
Depth of Hardening
Size change in hardening
Resistance to decarburization
what is secondary hardening?
the unintentional increase of hardness during tempering or machining of some hardened high alloy steel
Depth of Hardening
through hardening, Hardenability
Size change in hardening
Very important for design
what is decarburization
if a steel with a relatively high carbon content (~1%) is heated in a furnace that has a carbon-free atmosphere (air), carbon will tend to diffuse out of the steel
Hardening- Use Characteristics
Resistance to heat softening
Wear Resistance
Toughness
Machinability
Resistance to heat softening
the capability of an alloy to maintain its strength when exposed to high temperature
Wear resistance
a material's ability to resist material loss by some mechanical action
Toughness of tool steels
All tool steels have little or no toughness, some are just worse than others
Machinability
the ease with which the material is machined in terms of specific energy, specific horsepower, or shear stress
Body Centered Tretraganol
BCT
Elongated compared to BCC
BCC has low carbon content, BCT has carbon stuck in it because of rapid cooling
Martensite is this
Acicular
needle like structures
microstructure of martensite
Martensite has:
High tensile & high hardness
lowest ductility & lowest impact strength
Heat treatments (7)
Tempering
Hardening
Austempering
Stress Relieving
Spheroidizing
Martempering
Annealing
Normalizing
Tempering process
The normal procedure for tempering is to quench the part; while it is still warm, it is put in a furnace at the desired tempering temperature. When temperature sensors indicate that the partis at temperature, it is soaked for about 2 h and then air cooled.
800-1000 F; air cool
Tempering purpose
used to improve the toughness of quench-hardened steels
Stress relieving
reduction of internal strains leftover from another process by application of energy stress
900-1250 F
1 hr/inch of thickness; air cool
Spheroidizing process
Raise to temp right before austenite transition temp and then hold it there for very long which releases carbon from BCT, change to BCC ferrite + cementite spheroids
Makes "spheroidized Martensite" (No actual martensite in it; composed of BCC ferrite + cementite spheroids)
(1200 F; 96+ hrs)
When is spheroidizing used and what is the effect
Used if we tempered much to long
Improves machinability & resistance to fracture (type of annealing)
Austempering
Stops quench cracks & hardens material
cool in two steps
-first cool in molten salt (high liquid temp)
-then cool in water
Makes bainite
-looks like very tempered martensite(very hard)
Martempering
2 stages of cooling
-Molten salt bath with lower temp than austempering
-cool in water
Makes untempered martensite
*in order to get martensite, Austenite must be made first*
Flame hardening system
Martensite on just the surface
Selective hardening- works best with medium carbon steel
martensite on outside, ferrite & pearlite on inside
Difusion
Change chemistry of surface while solid
low carbon and low alloy steels
Must have this to occur:
*-difference in concentration*
*-material with low carbon*
Carburizing (diffusion)
Pack metal in carbon or carbon based gas and heat it up so that the metal soaks up carbon
two types:
-pack
-gas
Surface Hardening:
Carbonitriding (diffusion)
diffusion of carbon plus nitrogen into a steel surface
Nitriding (diffusion)
-Just like carburizing, but use nitrogen instead
-dont go nearly as hot (nitrogen can get in without steel being FCC(can stay BCC))
-Nitrides end up on surface (very hard & unwearable)
-Dont need to temper
-Brittle white layer that must be removed after nitriding process
-takes longer than carburizing
-thickness is smaller than carburizing
-no grain growth in nitriding, only in carburizing
Manganese (identification)
13xx
15xx
Nickel (identification)
23xx
25xx
Nickel-Chromium (identification)
31xx
33xx
Molybdenum (identification)
40xx
41xx Chromium & Molybdenum
43xx Nickel & Chromium
46xx
48xx
Chromium (Identification)
51xx
52xx Chromium
Chromium-vanadium (identification)
61xx
Multiple Alloy (identification)
86xx, 87xx, 92xx, 93xx, 94xx, 94Bxx
Carbon Steel
SAE 1006-1095 General Purpose
SAE 1108-1151 Free Machining
SAE 1513-1572 High Manganese
A611, A619, A620 ASTM Grades
Aluminum
(Al)
Aids nitriding
Restricts Grain Growth
Removes oxygen in steel melting
Sulfur and Phosphorus
(S & P)
Adds Machinability
Reduces Weldability, ductility, & toughness
Increases resistance to corrosion & oxidation
Chromium
(Cr)
Increases hardenability (big effect)
Increases high temp strength
Can combine with carbon to form hard, wear resistant microconstituents
Nickel
(Ni)
Promotes an austentic structure
Increases Hardenability (mild effect)
Increases toughness
Copper
(Cu)
Promotes tenacious oxide film to aid atmospheric corrosion resistance
Manganese
(Mn)
Increases hardenability
lowers hardening temp
promotes an austenitic structure
combines with sulfur to reduce its adverse effects
Silicon
(Si)
Removes oxygen in steel making
Improves toughness
Increases hardenability
Molybdenum
(Mo)
Promotes grain refinement
Increases hardenability
Improves high temp strength
Vanadium
(V)
Promotes grain refinement
Increases hardenability
Will combine with carbon to from wear resistant microconstituents
Boron
(B)
Added in small amounts to increase hardenability by alot
if too much added, reduces ductility(makes brittle)
Lead
(Pb)
Added only to aid in machinabiility
Nitrogen
(N)
Acts like carbon in strengthening
Carbon Equivalent Definition
the sum of the alloy additions that promote hardening similar to carbon
Carbon equivalency equation
%C + %Mn/6 + %Ni/15 + %Cr/5 + %Mo/4 + %V/4 + %Cu/15
Carbon Equivalency & weldability
When carbon equivalentcy is >.3%, weldability can be a problem because alloy steels have a higher hardenability than carbon steels
Normalizing
heating a steel to the fully austenite region, soaking at this temp, & air cooling to room temp
makes grain size & alloy distribution more uniform
900-1400 F
Annealing
Heating a steel to its austenitizing temp and then cooling it at a slow enough rate to prevent the formation of a hardened structure
cool at 100F/hr - 30F/hr
Increases machinability (softens a metal)
Hardening
Quenched after austenitizing temp is reached
high strength and toughness
as tempreing temp ___, hardness ____
increases, decreases
Microstructure types (4)
Ferrite
Austenite
Cementite
Martensite
Ferrite properties
Soft, ductile, magnetic
Austenite properties
Soft, moderate strength, non magnetic
Cementite properties
Hard, brittle
Martensite properties
Hardest
Hardenability definition
Ability of a steel to be hardened
What affects hardenability
alloy chemicals added, temperature, grain size
Quench Mediums (5) and order of severity
Quickest cool/most severe
Water->oil->salt bath->gas->air
What is OQT?
Oil quenched and tempered
What microstructure does OQT indicate for a low carbon steel?
Martensite
What microstructure does OQT indicate for a hypereutectoid steel?
Martensite and Cementite
Low carbon steel %
Medium carbon steel %
.3%-.6%
High carbon steel %
.6%-2%
Carbon steel definition
An alloy of iron and carbon with carbon below 2%
Corrosion
deterioration of a material or its properties because of reaction with its environment
problems caused by corrosion
weight gain/reduction, mechanical properties affected
Factors affecting corrosion (3)
environment
material properties
physical conditions
Requirements for corrosion to occur
anode (higher energy, active)
cathode (lower energy, passive)
metal path
electrolyte that will carry ions
difference in energy between anode & cathode
8 Basic types of corrosion
-uniform
-pitting
-crevice
-galvanic
-stress corrosion cracking
-intergranular attack
-dealloying
-erosion
what is slurry erosion
material removal due to the combined action of corrosion and wear. The source of the wear and an accelerator of the corrosion is abrasive particles dispersed in a slurry.

anode = (high energy/active OR low energy passive)
cathode = (high energy/active OR low energy passive)
anode (higher energy, active)
cathode (lower energy, passive)
3 ways to control corrosion
design
environment control
material selection
electrolyte
liquid or other medium that carrys current
electrochemical corrosion process
changes of state aided by electron/ion movement(conduction)
Galvanic cell
An electrochemical cell which converts the free energy of a chemical process into electrical energy