terms

0.0(0)
Studied by 0 people
call kaiCall Kai
learnLearn
examPractice Test
spaced repetitionSpaced Repetition
heart puzzleMatch
flashcardsFlashcards
GameKnowt Play
Card Sorting

1/35

encourage image

There's no tags or description

Looks like no tags are added yet.

36 Terms

1
New cards

Casting

A dependable process that allows you to create complex shapes with simple tools and practically any material with little waste.

2
New cards

Misrun

Happens when pouring material slowly; mold cools too quick

3
New cards

Cold shut

Cracks; happens when material poured too slow

4
New cards

Small riser

Material shrinkage not fully accommodated. Shrinkage occurs in heavier sections

5
New cards

Shrinkage allowance

Pattern allowance that compensates for contraction of material during solidification

6
New cards

Draft allowance

Pattern allowance that correlates to a tapered surface in the pattern to allow for easy removal of the cooled part

7
New cards

Machining allowance

Pattern allowance where extra material is added to a casting pattern to be machined later

8
New cards

Rapping

Pattern allowance where pattern is made smaller to accommodate for mold cavity enlargement for easy removal

9
New cards

Distortion allowance

Pattern allowance where uneven cooling & stresses are accommodated for by modifying the casting pattern

10
New cards

Cylindrical sprue

Bad. High velocity causes aspiration and casting defects

11
New cards

Sand moulding

Low cost, rough surface finish, uses sand, large castings

12
New cards

Shell moulding

High cost, smooth surface finish, uses resin-sand shells, smaller castings

13
New cards

Chill

Conducts heat away from isolated sections to promote uniform cooling & prevent defects

14
New cards

Grey cast iron

High compressive strength, machinability, vibration dampening, corrosion resistance

15
New cards

White cast iron

High hardness, wear resistant, brittle, poor machinability

16
New cards

Malleable cast iron

Heat treated white cast iron; tough, strong, and ductile

17
New cards

Nodular cast iron

Cast iron treated to promote strength & flexibility; high ductility, toughness, and tensile strength

18
New cards

Alloy cast iron

Cast iron with improved strength, heat resistance, and wear resistance

19
New cards

Investment pattern materials used because they are:

Disposable and easily removable before pouring cast

20
New cards

Core prints should be used over chaplets because:

Chaplet fusion is typically difficult and considered to be a defect

21
New cards

Gating ratio

Controls molten metal flow; sprue bottom area : runner area : ingate area

22
New cards

Cuts & washes (defect)

Material erodes sand during casting process

23
New cards

Fusion (defect)

Sand fuses to material during casting process

24
New cards

Swells (defect)

Casting surface enlarges during solidification

25
New cards

Runout (defect)

Material leaks from casting cavity

26
New cards

Drops (defect)

Sand falls into casting material before fully solidifying

27
New cards

Penetration (defect)

Metal enters sand of mold before solidifying

28
New cards

Rat tails (defect)

Cracks in casting following solidifying

29
New cards

Properties of sand

Hot strength, permeability, refractoriness, collapsibility, cohesiveness, adhesiveness

30
New cards

Die casting pros & cons

Highly accurate, great surface finish, rapid production, high strength.

Must be done in high volume, materials limited, high costs

31
New cards

Die casting pros & cons

Highly accurate, great surface finish, rapid production, high strength.

Must be done in high volume, materials limited, high costs

32
New cards
33
New cards

Hot tears (defect)

Cracks; occurs when casting shrinks but the internal stresses are not resolved

34
New cards

Why is investment casting preferred for complex shapes?

Complex geometries can only be made via investment casting with high quality & accuracy

35
New cards

Flash (defect)

Excess metal forming on parting line

36
New cards

Mismatch (defect)

Top and bottom halves of casting misaligned