MMET 207 Lab Final

0.0(0)
Studied by 0 people
call kaiCall Kai
learnLearn
examPractice Test
spaced repetitionSpaced Repetition
heart puzzleMatch
flashcardsFlashcards
GameKnowt Play
Card Sorting

1/79

encourage image

There's no tags or description

Looks like no tags are added yet.

80 Terms

1
New cards

What is the reason for hardness testing?

to measure a metal's resistance to indentation

2
New cards

What are the three methods of hardness testing?

Rockwell, Brinell, and Vickers

3
New cards

What is the minor load for the regular scale?

10 kg

4
New cards

What is the minor load for the superficial scale?

3 kg

5
New cards

What are the major loads for regular scale Rockwell?

60 kg, 100 kg, and 150kg

6
New cards

What are the major loads for superficial scale Rockwell?

15 kg, 30 kg, and 45 kg

7
New cards

What are the two types of indentors?

diamond cone (brale) or hardened steel ball

8
New cards

What is the notation for Rockwell A?

HRA

9
New cards

When is the minor load applied in hardness testing?

while zeroing the scale

10
New cards

What composes an HRA reading?

diamond indentor, 60 kg major load

11
New cards

What composes an HRC reading?

150 kg major load, diamond indentor

12
New cards

What Rockwell scales use the superficial scale?

N and T

13
New cards

What are the steps to tensile testing?

1. place machined specimen in tensile tester

2. apply tensile load, increasing until sample breaks

3. during loading, at intervals measure tensile load and length

4. after the sample breaks, but the broken ends together and measure length

14
New cards

How is stress calculated?

force/area

15
New cards

How is strain calculated?

(final length-original length)/ original length

16
New cards

What is the modulus of elasticity?

stress/strain in the straight line portion of graph; can't calculate when the graph isn't straight

17
New cards

What is percent elongation?

final strain *100%

18
New cards

What is the proportional limit?

when the behavior is elastic but not proportional

19
New cards

What is the yield strength?

when the material begins plastic deformation

20
New cards

What is the tensile strength or UTS of a material?

the highest strength achievable

21
New cards

What is the breaking strength?

the strength when the material breaks

22
New cards

What is ductility?

stretch, related to percent elongation

23
New cards

Modulus of elasticity measures what?

stiffness of a material

24
New cards

How do you find the 0.2% offset?

go to 0.2 on the strain axis (X) and draw a line that's parallel to the modulus of elasticity

25
New cards

What was the type of impact test used?

Charpy V notch

26
New cards

What was the impact testing machine set to before each test?

maximum value

27
New cards

What is the value that is shown after a specimen is broken during an impact test?

the absorbed energy in ft.lbs

28
New cards

What was the basic concept behind the impact testing lab?

to test the impact strength of samples at different temperature and plot them on a graph

29
New cards

When plotting the graph for ductile to brittle transition temperature, what should the axis' be labeled?

temperature on x, impact strength on y

30
New cards

What is ductile to brittle transition temperature?

the temperature at which the fracture energy passes below a predetermined value

31
New cards

What type of materials have ductile to brittle transition temperatures?

BCC materials

32
New cards

A 36

ferrite and pearlite

33
New cards

Gray Cast Iron (GCI)

ferrite, pearlite and graphite flakes

34
New cards

1095 Water Quenched and Tempered

martensite, ferrite and cementite

35
New cards

4340 A

ferrite and pearlite

36
New cards

Ductile Cast Iron

ferrite, pearlite and graphite spheroids

37
New cards

4340 WQ

martensite

38
New cards

Pig Iron

pearlite, cementite, and graphite flakes

39
New cards

Malleable Cast Iron (MCI)

ferrite and graphite nodules

40
New cards

1095 AC

pearlite and cementite

41
New cards

White Cast Iron (WCI)

pearlite and cementite

42
New cards

1095 WQ

martensite and cementite

43
New cards

Speroidized MArtensite

cementite spheroids and ferrite

44
New cards

Wrought Iron

ferrite and iron silicate stringers

45
New cards

Pack Carburized Steel

two outer layers-martensite and cementite

two inner layers-ferrite and pearlite

46
New cards

What is the echant composed of?

95% alcohol and 5% nitric acid

47
New cards

What is important to remember when mixing the echant?

always add the acid

48
New cards

What is the polishing media for metallography?

alumina or aluminum oxide

49
New cards

What are the sizes that the polishing media come in?

1, 0.3, and 0.05 michron

50
New cards

What are the order of the grit stages on the sandpaper used for etching?

240, 320, 400, and 600

51
New cards

What were the steels that were used during heat treating?

1018, 4340, and 52100

52
New cards

What were the three quench methods that were used in heat treating?

water, air, oil

53
New cards

What cooling method results in the hardest material?

water quench

54
New cards

What cooling method results in the least hard material?

air quench

55
New cards

How do tempering temperatures affect the material's hardness?

increases ductility, decreases tensile strength, increases impact strength and decreases hardness

56
New cards

Heating and cooling cycle for hardening

1650-1700 degrees F for 1hr/in of thickness; quench

57
New cards

Heating and Cooling cycle for tempering

800-1000 degrees F for 2 hours; air cool

58
New cards

Heating and Cooling cycle for annealing

1650-1700 degrees F for 1 hr/in of thickness; furnace cool

59
New cards

How was the lead-tin solidification diagram plotted?

x-axis was time, y-axis was temperature in degrees C

60
New cards

What is undercooling?

where the liquidus line dips down into the solid region

61
New cards

How is pack carburizing done?

a sample of low carbon steel is placed in a carbon rich material, activated charcoal, and is heated, so that the carbon diffuses into the steel

62
New cards

What are the temperatures and time for pack carburizing?

1650 degrees F for 8 hours

63
New cards

What is the grain size after pack carburizing?

large, and it must be refined

64
New cards

What is the two step heat treating process to refine grains?

first, you heat to 1650 for 30 minutes for small grains in the core and then to 1400 for 20 minutes for small grains in the case

65
New cards

What kind of stainless steel was tested during the cold working lab?

Austenitic stainless steel

66
New cards

What is the crystal structure of austenitic stainless steel?

FCC

67
New cards

As thickness of austenitic stainless steel was reduced, what happened to the hardness and magnetism?

they both increased

68
New cards

What effect did the two cooling rates have on the hardness after heat treating?

they both did not increase hardness since there is not a phase change to allow martensite to form

69
New cards

What happened to the hardness and magnetism after heat treating?****

they were lowered because of the recrystallization that occured

70
New cards

What should you do to the metal sample while grinding them in the metallography lab?

rotate it 90 degrees so that the replacement of scratches can easily be seen

71
New cards

What are the settings to the mounting press used for metallography?

use 1.25" mold with 4200 psi

72
New cards

What media was put into the mold for the metallography lab?

Phenolic or bakelite powder

73
New cards

DBTT

Ductile to brittle transition temperature

74
New cards

What should you do after you've finished grinding a metal sample with all 4 sand papers?

don't touch it with your fingers

75
New cards

Why is jominy testing used?

to determine the effect of alloying elements on microstructure development at different cooling rates

76
New cards

What were the major alloying elements in the samples used in jominy testing?

Chromium, Molybdenum, and Nickel

77
New cards

What were the three materials tested in jominy testing?

1045, 4140, 4340

78
New cards

How were the plots graphed for jominy testing?

distance from quenched end vs. HRA

79
New cards

Which sample from jominy testing had the highest hardenability?

4340

80
New cards

What is the most widely used hardness test?

Rockwell