1/97
Looks like no tags are added yet.
What is adhesion?
The process of holding two surfaces/materials together.
What is an adhesive?
A material used to bond two surfaces together.
What are adherends?
The two surfaces or materials being joined by an adhesive.
What is adhesive bond strength?
How strongly the adhesive sticks to the surface at the interface.
What is cohesive bond strength?
How strongly the adhesive holds together within itself.
What is the difference between adhesive and cohesive failure?
Adhesive failure separates at the surface/adhesive interface. Cohesive failure splits within the adhesive.
What three things help an adhesive form a good bond?
It must wet the surface, flow into surface irregularities, and be chemically compatible with the materials.
What is wettability?
How easily a liquid adhesive spreads across a surface.
What does a low contact angle mean?
The liquid spreads out more, indicating better wetting.
What does a high contact angle mean?
The liquid beads up more, indicating poorer wetting.
What contact angle generally indicates wetting?
A contact angle below 90 degrees indicates wetting; a smaller angle means better spreading.
What surface-tension relationship helps an adhesive wet a solid?
The adhesive's surface tension should be lower than the solid's critical surface tension; the lecture rule is about 10 dynes/cm lower.
Which polymer in the practice values has very low surface energy and is difficult to wet?
PTFE (Teflon), with a critical surface tension around 18 dynes/cm.
What is solubility parameter used for when choosing adhesives?
It helps predict chemical compatibility between materials.
What does a small difference between two solubility parameters indicate?
The materials are more compatible; similar values (δ1 approximately equals δ2) are preferred.
What does a large difference between solubility parameters indicate?
The materials are less compatible.
What is viscosity?
A liquid's resistance to flow; higher viscosity means thicker flow.
How does low viscosity affect adhesive application?
It flows and spreads more easily.
How does temperature affect hot-melt adhesive viscosity?
As temperature increases, viscosity decreases.
How does molecular weight affect viscosity?
As molecular weight increases, viscosity generally increases.
How does dissolving adhesive in a liquid affect viscosity?
It lowers application viscosity, making the adhesive easier to spread.
What is a hot-melt adhesive?
An adhesive applied while melted that forms a bond as it cools; it is 100% solids and uses no solvent.
What common polymer is used in many hot-melt adhesives?
EVA (ethylene-vinyl acetate).
What is a solvent-borne adhesive?
A polymer adhesive dissolved in an organic solvent; the solvent must be removed after application.
What is a water-borne adhesive?
An adhesive carried or dispersed in water, often as an emulsion.
What is a reactive adhesive?
An adhesive that chemically reacts or crosslinks to develop its final bond properties.
What is a pressure-sensitive adhesive (PSA)?
An adhesive that remains tacky and bonds when pressure is applied, commonly used for labels and tapes.
Why does a PSA often use a release liner?
The liner prevents the tacky adhesive from sticking before it is ready to be applied.
What is a cold-seal adhesive?
A pressure-activated adhesive that seals to itself without heat; commonly used for food/candy wrappers.
What is latex in adhesive terminology?
A dispersion of polymer particles in a liquid, usually water.
What is an emulsion?
A suspension or dispersion of adhesive solids in a fluid.
What is solids content?
The amount of solid material remaining after solvents or liquids are removed.
What is setting time?
The time required for an adhesive to form a bond.
What is open time?
The time between applying the adhesive and bringing the substrates together.
What is tack?
The stickiness of an adhesive and its ability to form an initial bond immediately.
What is shortness?
A lack of stringing when an adhesive is applied or pulled apart.
What is heat sealing?
Joining materials using heat and pressure, with at least one thermoplastic heat-seal layer.
What is seal initiation temperature (SIT)?
The minimum temperature required to obtain an acceptable heat seal.
Why is a low SIT useful?
It takes less energy to start a seal and can allow faster packaging-line speeds or lower jaw temperatures.
What are the three regions of a heat-seal strength curve?
Seal initiation temperature, maximum-seal/plateau region, and seal-degradation temperature.
What is the seal temperature range/window?
The range of temperatures that produces acceptable seals.
Why is a broad seal-temperature window useful?
It gives more consistent seals despite variations in seal-jaw temperature and packaging-line speed.
What is ultimate seal strength?
The strength of the seal after the interface has cooled.
What is hot tack?
The strength of a seal immediately after sealing, while it is still hot and before cooling.
Why is hot tack important in form-fill-seal packaging?
The hot seal must resist forces from falling product, introduced air, or package spring-back before it cools.
What are the three seal properties that help packaging machinery run reliably?
Low seal initiation temperature, broad seal-temperature range, and high hot-tack strength.
What is heated-bar sealing?
A method that uses heated bars/jaws and pressure to form a seal.
What is impulse sealing?
A method where the heating element is energized for a short interval during the sealing cycle rather than being continuously hot.
How does induction sealing work?
An electromagnetic field induces current in a metal foil liner; the foil heats and transfers heat to the sealant, bonding it to the container rim.
What is adhesive peel?
A peel failure between adjacent layers without tearing either polymer layer; the adhesive remains on one substrate.
Where is adhesive peel desirable?
Clean-peel packages such as medical tray lids, cereal packages, and coffee packages.
What is cohesive peel?
The sealant splits internally, leaving some adhesive/sealant material on both sides.
What is a tear seal or substrate failure?
The substrate itself tears during separation; it can provide tamper evidence.
What is delamination peel?
Separation of layers within a laminate structure.
What is extrusion?
A process that melts plastic and pushes it through a die to create a continuous shape such as film.
What does the hopper do on an extruder?
It holds and feeds plastic pellets into the extruder barrel.
What does the feed zone of an extruder do?
It conveys the pellets forward and begins compacting them.
What does the compression/transition zone do?
It compresses the material, helps melt the pellets, and squeezes out air as the screw channel becomes shallower.
What does the metering zone do?
It makes the melt more uniform and pushes it forward at a steadier rate and pressure.
What does the die do in extrusion?
It shapes the molten polymer as it exits the extruder.
What generally happens to polymer temperature along an extruder?
The material is heated and melted as it moves through the barrel; the exact temperature profile depends on the polymer and process.
What is the main advantage of a twin-screw extruder over a single-screw extruder?
Better mixing of polymer components and additives.
Why is it inaccurate to say single-screw extruders are excellent mixers and need no special mixing devices?
Single-screw extruders mainly convey and melt; mixing may require special screw sections or mixing devices.
How is cast film made?
Molten polymer exits a flat/slot die, is cooled on chill rolls or in a quench bath, then pulled by rolls and wound.
What are common cast-film characteristics from the lecture?
Good transparency and stiffness; film may be narrower than the die and thicker at the edges due to thermal contraction and elastic relaxation.
How is blown film made?
Melt exits an annular/circular die as a tube, air inflates it into a bubble, the bubble is air-cooled and collapsed by pinch rollers, then wound or slit.
What are common blown-film characteristics from the lecture?
Generally hazier, less transparent, less uniform in gauge, and more variable in thickness; it has greater crystallinity and better barrier properties.
What controls blown-film properties?
Blow-up ratio and linear line speed.
What is MD?
Machine direction: the direction the film travels during manufacture.
What is CD?
Cross direction: the direction across the width of the film.
What is film orientation?
Stretching film so polymer molecules become aligned in the direction of the stretch.
How does orientation affect film properties?
It increases strength, crystallinity, and barrier properties in the stretched direction, while strength decreases in the perpendicular direction.
What is uniaxial orientation?
Stretching the film significantly in one direction.
What is biaxial orientation?
Stretching the film in both machine direction and cross direction.
Why are multilayer films used?
They combine properties such as moisture resistance, oxygen barrier, toughness, heat sealability, appearance, and machinability.
What is coextrusion?
Making a multilayer film in one step by melting different resins in separate extruders and bringing the melts together in or before one die.
In coextrusion, do the polymers exist as separate webs before joining?
No. The melts join during the process; the materials do not exist as separate webs first.
Do coextruded layers mix into one homogeneous material?
No. They remain as distinct layers; the goal is stable, separate layers rather than mixing.
What factors must be considered in coextrusion?
Polymer flow/rheology, melt-viscosity matching, keeping layers from intermingling, layer uniformity, and adhesion between layers.
What is a tie layer?
A functionalized resin layer that acts like an adhesive between polymers that do not naturally adhere well, often polar and nonpolar resins.
What is coating?
Applying a relatively thin layer of material onto at least one substrate/web.
What is lamination?
Bonding two or more webs together to create one combined web.
Why can coating be less costly than lamination?
A coating is generally thinner than the lightest separate film that could provide the same function.
What is extrusion coating?
Applying a molten thermoplastic layer onto a substrate web such as paper.
What is extrusion lamination?
Adding a second web and bonding both webs using the adhesive action of the extruded molten thermoplastic.
What does neck-in mean in extrusion coating?
Contraction or narrowing of the molten polymer curtain in the cross direction.
What is adhesive lamination?
Applying adhesive to one web and then joining it to a second web.
What is dry-bonding lamination?
Apply adhesive to the first substrate, dry/remove its solvent, then join the second substrate using a heated nip.
What is wet-bonding lamination?
Join the two substrates while the adhesive is still wet, then pass them through an oven to set the adhesive.
Why must one web be porous in wet-bonding lamination?
The porous web allows adhesive solvent or water to escape.
What is a Mayer rod coater?
A wire-wound rod that meters the coating and removes excess liquid from the web.
What is a gravure roll coater?
An engraved-cell roll that transfers a controlled amount of coating to the web; a doctor blade removes excess coating.
What is metallization?
Depositing a very thin metal layer, commonly aluminum, onto a film or substrate to create a metallic appearance and improve barrier properties.
What is silicon oxide (SiOx) coating used for?
A thin glass-like coating that improves barrier properties while retaining more transparency than a metal layer.
What are the likely functions of the layers in LDPE/paper/LDPE/foil/LDPE (outside to inside)?
Outer LDPE: protection/moisture resistance; paper: stiffness and printability; middle LDPE: bonding/moisture barrier; foil: light, oxygen, and moisture barrier; inner LDPE: heat-seal/product-contact layer.
What is the correct yield for 200-gauge (2 mil) PVC with specific gravity 1.35?
Approximately 146 cm²/g.
What is the density of a material with specific gravity 1.35?
Approximately 1.35 g/cm³, assuming water density is 1 g/cm³.
How do you calculate film yield?
Convert thickness to cm; multiply thickness by density to get mass per cm²; divide 1 cm² by that mass to get cm²/g.