1/23
Looks like no tags are added yet.
What factors cause variability in wood strength testing?
Moisture content, specific gravity, defects and variation of properties within the same species.
What ASTM standard governs the testing of small clear wood specimens?
ASTM D143.
What are the four purposes of testing wood under ASTM D143?
Compare mechanical properties between species, establish allowable design stresses, relate mechanical properties to physical properties and measure the influence of defects.
What is the loading rate for tension testing parallel to the grain?
1 mm/min.
Why are tension-parallel-to-grain test specimens designed with wider ends?
To prevent the specimen ends from pulling away from the grips or crushing during testing.
What happens during tension testing perpendicular to the grain?
The growth rings are pulled apart against the lignin matrix.
What is the loading rate for tension testing perpendicular to the grain, and why is this test of limited design significance?
2.5 mm/min; wood is generally not designed to resist tension perpendicular to the grain.
What is the loading rate for the static bending test of wood?
2.5 mm/min.
What are the specimen dimensions and support span illustrated for the static bending test?
5 in × 5 in cross section, 70 in support span and 3 in overhang at each end.
What physical property must be measured after the static bending test?
Moisture content.
What is the purpose of the load-deflection curve in static bending testing?
To evaluate bending behavior and determine modes of failure.
What is the difference between brash failure and splintering failure?
Brash failure is abrupt; splintering failure is fibrous.
Why is static bending one of the most important wood tests?
Wood is commonly used for structural beam elements.
How does a knot affect stress distribution in a wood specimen?
It creates stress concentrations around the defect.
What are the specimen dimensions for compression testing parallel to the grain?
5 cm × 5 cm × 20 cm.
What is the loading rate for compression testing parallel to the grain?
0.03 cm per cm of specimen length per minute.
What is the loading rate for a 20 cm specimen undergoing compression testing parallel to the grain?
0.03 × 20 = 0.6 cm/min, or 6 mm/min.
How are failures classified during compression testing parallel to the grain?
According to the appearance of the fracture surface; if multiple failure types occur, describe them in their order of occurrence.
Where is moisture content measured after compression testing parallel or perpendicular to the grain?
Near the failure surface or region.
What is the loading rate for compression testing perpendicular to the grain?
0.3 mm/min.
What is the significance and failure mechanism of compression testing perpendicular to the grain?
Evaluates resistance to crushing at beam supports or locations of heavy applied loads; failure occurs through crushing and lateral collapse of fibers.
What is the loading rate for shear testing parallel to the grain according to ASTM D143?
6 mm/min.
What is the significance of shear testing parallel to the grain?
Determines wood shear strength, particularly horizontal shear resistance in short-span deep beams and the shear strength of glulam.
How is the wood impact test performed and what property does it measure?
Drop a 22.5 kg weight from heights increasing in 2.5 cm increments until failure or 15 cm deflection; measures toughness, and moisture content is recorded.