1/21
Looks like no tags are added yet.
α - Iron
Ferrite (BCC) → Low carbon solubility
γ (gamma) -
Austenite (FCC) → much higher solubility
δ - Iron
δ Ferrrite (BCC) → exists at very high temps
Fe3C
Cementite (Orthorhombic) →Hard, brittle iron carbide
Eutectic Reaction
L <→ Y + Fe3C (occurs at 4.3 wt% C and 1147oC)
Eutectoid Reaction
Y ←> α + Fe3C (occurs at 0.76 wt% C and 727°C)
Commercially pure iron
Below 0.008 wt%
Steel
0.008–2.14 wt%
Cast iron
2.14–6.70 wt%
When eutectoid steel (0.76wt% C) is cooled below 727oC?
All austenite (Y) transforms into alternating layers of ferrite (α) and cementite (Fe3C), forming pearlite.
What is pearlite?
A microconstituent consisting of alternating layers (lamellae) of ferrite and cementite. (cementite layers are 1/8 the thickness of ferrite)
Why does pearlite form in alternating layers?
allows for redistribution of carbon by diffusion
Hypoeutectoid Alloy
an alloy with a carbon content below the eutectoid composition. (0.0022-0.76 wt% C)
Development of hypoteuctoid steel during slow cooling
Initially all austenite (Y)
Proeutectoid ferrite (α) forms at grain boudaries
Below 727oC, all remaining austenite transforms into pearlite
What is proeutectoid ferrite?
Ferrite that forms before the eutectoid reaction, rather than as a part of pearlite.
Why does ferrite (α) formation start at grain boundaries?
Results in smaller increase in the interfacial energy.
what is a hypereutectoid alloy
An alloy with a carbon content above the eutectoid composition (0.76-2.14 wt% C for the steels discussed)
Development of hypereutectoid steel during slow cooling
Initially all austenite (Y)
Proeutectoid cementite (Fe3C) forms at grain boundaries
Below 727o, all remaining austenite transforms into pearlite
What is proeutectoid cementite?
Cementite that forms before the eutectoid reaction, rather than as a apart of pearlite.
Main difference between hypoeutectoid and hypereutectoid microstructure development?
Hypoeutectoid: ferrite forms first
Hypereutectoid: cementite forms first
In both: remaining austinite becomes pearlite
What happens to all the remaining austenite when cooling across the eutectoid isotherm
It turns into pearlite (in all cases)
reasons to alloy
improved corrosion resistance
better machinability
better heat treatment