When were acrylic polymers first introduced as denture base materials?
1937
What are the highlighted focus areas of polymers in dentistry?
Fixed and removable prosthodontics
What are examples of polymers in fixed prosthodontics?
Cements; Impression trays; Impression materials; Temporary crowns
What are examples of polymers in removable prosthodontics?
Impression trays; Impression materials; Denture bases; Denture teeth
What are the classifications of denture base resins? **
Self cured
Heat cured
Light cured
Microwave activated
Laser activated
What are the requirements of denture base resins? **
Tasteless, odorless, non-toxic, non-irritant
Aesthetically satisfactory
Color stability
Insoluble and impermeable to oral fluids
Low specific gravity [light weight]
Should tolerate the temperature of food
Dimensional stability
Easy to fabricate and repair
Should have enough strength, resilience, and abrasion resistance
Good thermal conductivity
What is the powder component of denture base resin?
Poly methyl methacrylate and other co-polymers - dissolved by monomer to form the dough
Benzoyl peroxide - initiator
Compound of mercuric sulfide [or] cadmium sulfide - dyes
Zn or Ti oxide - opacifier
Dibutyl phthalate - plasticizer
Dyed organic fibers
Esthetics - inorganic particles
What is the liquid component of denture base resin?
M.M.A. - monomer
Dimethyl para toluidin – activator
Dibutylphthalate - plasticizer
Glycal dimethacrylate - cross-linking agent
Hydroquinone - inhibitor
What are the curing methods of acrylic polymers and their activation?
Heat cure: heat activation; Chemical cure: chemical activation; Light cure: light-activated photoinitiator
What are the liquid components of heat-cure acrylic resin shown in the lecture?
MMA; Hydroquinone
What are the powder components of heat-cure acrylic resin shown in the lecture?
PMMA; Fillers; Dyes; Benzoyl peroxide
What are the liquid components of chemical-cure acrylic resin shown in the lecture?
MMA; Hydroquinone; Accelerator (tertiary aromatic amine)
What are the powder components of chemical-cure acrylic resin shown in the lecture?
PMMA; Fillers; Dyes; Benzoyl peroxide
What are the components of the light-cure acrylic resin putty system shown in the lecture?
MMA / PMMA; Fillers; Dyes; Camphorquinone (photo initiator)
What are the processing stages shown for acrylic polymers?
Mix → dough formation; Packing stage; Polymerized
What are the melting point and boiling point of MMA shown in the lecture?
Melting point - 48 ° C; Boiling point ~ - 100 ° C
What is the volumetric shrinkage of MMA?
21%
What is the modulus of elasticity of MMA?
2200 MPa
What is the creep of MMA?
9 MPa
What are the physical properties of polymethylmethacrylate (PMMA)?
Clear, transparent, can be pigmented - pink, white, tooth colour, transparent
What is the density of PMMA?
1.19gm/cm cube
What is the compressive strength of PMMA?
75 MPa
What is the tensile strength of PMMA?
52 MPa
What is the impact strength of PMMA?
Low
What is the hardness of PMMA?
16-18 KHN
What is the modulus of elasticity of PMMA?
2400 MPa
What is the dimensional stability of PMMA?
Moderate
What are the steps in the conventional processing of an acrylic denture base?
PRELIMINARY IMPRESSION: Make an alginate impression of the patient's maxillary arch.
STUDY MODEL: Pour the impression in gypsum to produce the study cast.
CUSTOM TRAY AND FINAL IMPRESSION: Fabricate an acrylic-PMMA tray; make the final elastomeric impression.
RECORD BASE AND WAX RIM: Prepare the record base, establish jaw relations, and arrange the trial denture teeth.
FLASKING AND WAX ELIMINATION: Invest the waxed denture in gypsum; boil out and remove the wax.
PACK AND POLYMERIZE: Pack acrylic resin into the mold, cure, then deflask and finish the denture.
What is the typical heat-cure cycle shown in the processing diagram?
74 °C for at least 8 hours
What are the technical methods listed for acrylic denture base processing?
Compression moulding technique
Injection moulding technique
Fluid resin technique
Visible light curing technique
What are the steps in denture base resin processing?
Preparation of wax pattern
Preparation of split mould
Application of separating medium
Mixing of powder and liquid
Packing
Curing
Cooling
Deflasking, finishing, and polishing

What does the curing cycle refer to?
The heating process used to control polymerization.
What is Technique 1 for the curing cycle?
Heat in water bath at 74 degrees for 8 hrs with no terminal boiling.
What is Technique 2 for the curing cycle?
Heat at 74 degrees for 8 hr & then increase to 100 degrees for 1hr.
How should the flask be cooled?
bench cooled for 30 min - then immersed in cool tap water for 15 min.
What can rapid cooling cause?
Rapid cooling may result in warping of the denture base due to differences in the thermal contraction of the resin and investing stone.
Elastic modulus (stiffness) of acrylic (PMMC) denture base:
low
Impact strength of acrylic (PMMC) denture base:
moderate
Fatigue strength of acrylic (PMMC) denture base:
moderate
Water sorption of acrylic (PMMC) denture base:
high
Water soluabilty of acrylic (PMMC) denture base:
low
Thermal conductivity of acrylic (PMMC) denture base:
low
Polymerization shrinkage of acrylic (PMMC) denture base:
moderate to high (6% by volume)
Heat distortion temperature/glass transition temperature (Tg) of acrylic (PMMC) denture base:
is 95 °C
exposure to hot water can cause distortion and compromise fit.
Biocompatibility of acrylic (PMMC) denture base:
generally good
However, toxicity or allergic reactions if excessive residual monomer is present due to improper processing.
What are the uses of denture base resins listed in the lecture?
Denture base**
Record base**
Impression trays (custom tray)
Artificial teeth
Temporary crowns
Orthodontic appliances
Maxillofacial prosthesis