1/49
Looks like no tags are added yet.
What do we use ceramics to replace?
Enamel
Why is replacing enamel with ceramic necessary?
Withstands better forces without tooth being altered
Occlusion load of molars
400-800 N; 80 KgF/mm2
Occlusion load of premolars
220-450 N; 45 KgF/mm2
Occlusion load of caines
130-330 N; 33 KgF/mm2
Occlusion load of incisors
90-150 N; 15 KgF/mm2
What are the clinical indications of ceramics?
-Endodontically treated teeth
-Discolored teeth
-Broken teeth
Classes of ceramics
-Glass ceramics
-Polycrystalline
-Reinforced resin composite
Glass ceramics
-Feldspathics
-Leucite
-Lithium disilicate
-Lithium Silicate
Polycrystallines
-Alumina
-Zirconia
-Ytria-stabilized zirconia
Reinforced resin composite
-Resin infiltrates nanocera
-Ceramic-infiltrated
-Zirconia/silica-infiltrated
Feldspathics
-Thin and fragile
-Castable on metallic infrastructure
-Low compressive resistance
-Low flexural strength compared to the forces experienced by actual teeth (70MPa)
Leucite
-1st metal free crown
-Increased mechanical properties
-180 MPa flexural strength
Lithium Disilicate
-Particle size decreased allowing higher mechanical properties
-Metal-free over 3 elements (bridge)
-340 MPa flexural strength
Lithium silicate
-Glass predominance phase
-Reinforced with zirconia
-Silicate particle 6x smaller than disilicate particles (increased mechanical properties)
-500 MPa flexural strength
Two kinds of reinforced resin composite
Lava ultimate (ZIRCONIA)
Enamic (GLASS)
What are the different ways to produce ceramic materials?
-Layering and firing
-Heat pressing
-CAD/CAM milling
-3D printing
Layering and firing
-Porcelain powder and modeling liquid
-Incremental application
-Excellent individualization
-Highly technique and labor sensitive
Heat pressing
-Wax pattern is fabricated and sprued
-Pattern invested then goes through burnout
-Heat ceramic ingot is pressed into the mold
What are the drawbacks to heat pressing?
Can create voids or changes in dimensions leading to improper fit of restorations
Workflow of CAD/CAM milling
-Scan
-CAD/CAM
-Mill block
-Crystallize/glaze
-Final crown
What is an advantage to CAD/CAM blocks?
They are industrial blocks that provide standardizes material quality
How does the final crystallized state after crystallization and firing compare to the blue state in CAD/CAM?
-530 MPa flexural strength
-Shade and translucency develop (esthetic)
-Microstructure reaches final state
What are the concerns with additive manufacturing of ceramics?
Shrinkage, defects, porosity, and long-term clinical evidence
Cementation of ceramics utilizes what?
Micromechanical adhesion
What are the two means of curing in dual activation resin composite?
Light and chemical reaction
What is the photoinitiator that allows dual activation resin composite to cure via light?
camphorquinone
What triggers the chemical reaction cure in dual activation resin composite?
Benzoyl peroxide and aromatic tertiary amine
Why is the chemical polymerization slower than light curing in dual activation resin composite?
The chemical reaction produces free radicals
What are the benefits to using dual activation resin composite?
-Polymerization guarantee
-Work time
How long does it take for dual activation resin composite to polymerize?
5 min
What are the steps to conventional cementing on enamel?
-Phosphoric acid (etch)
-Primer
-Adhesive
How long does it take to conventionally cement enamel?
15-30 seconds
What is removed in the process of conventionally cementing enamel?
Biofilm
What is formed to increase contact area when conventionally cementing enamel?
Microretentions
What are the steps in conventionally cementing dentin?
-Phosphoric acid (etch)
-Primer + adhesive (one step together)
How long does it take to conventionally cement to dentin?
10-20 seconds
What is removed when conventionally cementing dentin?
smear layer
What does mineral dissolution lead to when conventionally cementing dentin?
-Exposure of collagen fibers
-Enlargement of the tubules
What is the difference between self-etching cements and conventional?
There is no bonding system in self-etching
What makes up the 10-MDP adhesive system?
-Chemical bonds
-Van der waals forces
-Hydrogen bonds
-Modified hybrid layer
-Absence of tags
What do we use hydrofluoric acid for?
GLASS ceramics
What does hydrofluoric acid do?
Exposes crystals in glass ceramics to then apply silane to create a bond between crystals and polymers
How long do you expose feldspathics to hydrofluoric acid?
60s
How long do you expose reinforced glass to hydrofluoric acid?
20s
Why is silane a bifunctional molecule?
Made up of an organofunctional group and aquila group
What is the organofunctional group in silane?
methacrylate
What is the aquila group in silane?
Si - O - Si (in ceramic)
Why should you wait 1 minute after applying silane before you apply the adhesive?
Wait for the chemical reaction to occur
Things to be aware of when apply adhesive with glass ceramics?
-Gently evaporate solvents
-Do NOT photoactivate
-Keep it protected from light