RCD - 1ST Week

0.0(0)
Studied by 0 people
call kaiCall Kai
learnLearn
examPractice Test
spaced repetitionSpaced Repetition
heart puzzleMatch
flashcardsFlashcards
GameKnowt Play
Card Sorting

1/57

encourage image

There's no tags or description

Looks like no tags are added yet.

58 Terms

1
New cards

Reinforced Concrete

A combination of concrete and steel wherein the steel reinforcement provides the tensile strength lacking in the concrete.

2
New cards

Joseph Lambot

In the mid-1800s, he constructed a small boat exhibited at the Paris Exposition of 1854 and received a patent in 1855 showing a reinforced concrete beam and column reinforced with four round iron bars.

3
New cards

Joseph Monier

An agriculturist who started experimenting with reinforced concrete containers in 1868 and built a bridge in 1875 at the Chateau de Chazelet, France, which led him to patent the concept of reinforced concrete beam.

4
New cards

Francois Hennebique

A French engineer who developed a scientific approach to the proportioning of concrete elements and helped make reinforced concrete a serious construction material in Europe.

5
New cards

Thaddeus Hyatt

Originally a lawyer, he was one of the earliest users of reinforced concrete in the United States, conducting experiments on reinforced concrete beams in the 1850s and investigating fireproof qualities.

6
New cards

William E. Ward

In 1870, he built the first landmark building structure in reinforced concrete in Port Chester, New York, known as the first reinforced concrete structure in the United States.

7
New cards

Ernest L. Ransome

In 1890, he built the Leland Stanford Jr. Museum in San Francisco and patented a system of ferro-concrete with iron rods twisted to improve the bond.

8
New cards

Concrete

A mixture of sand, gravel, crushed rock, or other aggregates held together in a rockpile mass with a paste of cement and water.

9
New cards

Cement

A material that has adhesive and cohesive properties enabling it to bond mineral fragments into a solid mass, which can set and harden in the presence of water.

10
New cards

Hydraulic cements

Cements of interest for reinforced concrete construction that can set and harden in the presence of water, consisting primarily of silicates and aluminates of lime.

11
New cards

Portland cement

The usual hydraulic cement used for reinforced concrete, named because of its resemblance when hardened to Portland stone found near Dorset, England.

12
New cards

Aggregates

Materials used in concrete that occupy about 75% of the concrete volume, including both fine and coarse types.

13
New cards

Fine aggregates

Any aggregate that passes a No.4 sieve (about 6 mm in size).

14
New cards

Coarse aggregate

Material of a larger size than a No.4 sieve (larger than about 6 mm).

15
New cards

Maximum size limit for coarse aggregates

Must not be larger than 1/5 of the narrowest dimension between the sides of the forms, 1/3 of the overall depth of slabs, or 3/4 of the minimum clear spacing between individual reinforcing bars.

16
New cards

Water requirement for concrete mixing

Shall be clean and free from injurious amounts of oils, acids, alkalis, and salts; non-potable water can be used if tests confirm it doesn't negatively affect setting times and durability.

17
New cards

Deformed bars

Reinforcing steel bars that have ribbed projections rolled into their surfaces to provide better bonding between the concrete and steel.

18
New cards

Plain bars

Reinforcing steel bars that are not used very often except for wrapping around longitudinal bars primarily in columns.

19
New cards

Admixtures

Materials added to concrete during or before mixing to improve its performance in certain situations or to lower its cost.

20
New cards

Air-entraining admixtures

A type of admixture added to concrete to improve its performance or lower its cost, which works by creating tiny air bubbles that provide space for water to expand when it freezes, thereby protecting the concrete from damage caused by freeze-thaw cycles and thermal expansion.

21
New cards

Accelerating admixtures

Additions (such as calcium chloride) that accelerate early strength development, particularly useful in cold climates, allowing for reduced curing times and earlier form removal.

22
New cards

Retarding admixtures

Additions (consisting of various acids or sugars/sugar derivatives) used to slow the setting of concrete and retard temperature increases, prolonging plasticity.

23
New cards

Superplasticizers

Admixtures made from organic sulfonates that enable engineers to reduce the water content substantially while increasing slumps, or to produce workable concretes with higher strengths while using less cement.

24
New cards

Waterproofing materials

Admixtures usually applied to hardened concrete surfaces or added to mixes, generally consisting of soap or petroleum products (like asphalt emulsion) to help retard water penetration into porous concretes.

25
New cards

Compressive Strength

The compressive strength of concrete, fc′, is determined by testing to failure 28-day-old 6 in. diameter by 12 in. diameter concrete cylinders at a specified rate of loading. For the 28-day period, the cylinders are usually kept under water or in a room with constant temperature and 100% humidity.

26
New cards

Stress-Strain Curve Linearity

The curves are roughly straight while the load is increased from zero to about one-third to one-half the concrete's ultimate strength.

27
New cards

Nonlinear Behavior

Beyond this range the behavior of concrete is nonlinear. This lack of linearity of concrete stress-strain curves at higher stresses causes some problems in the structural analysis of concrete structures because their behavior is also nonlinear at higher stresses.

28
New cards

Ultimate Strain

Regardless of strengths, all the concretes reach their ultimate strengths at strains of about 0.002.

29
New cards

Failure Strain

Concrete does not have a definite yield strength; rather, the curves run smoothly on to the point of rupture at strains of from 0.003 to 0.004. It will be assumed for the purpose of future calculations in this text that concrete fails at 0.003 (ACI 10.2.3).

30
New cards
31
New cards

Cylinder vs. Beam Behavior

Many tests have clearly shown that stress-strain curves of concrete cylinders are almost identical to those for the compression sides of beams.

32
New cards

Brittleness

It should be further noticed that the weaker grades of concrete are less brittle than the stronger ones—that is, they will take larger strains before breaking.

33
New cards

Limits for fc′​ (Normal-weight and lightweight concrete for general application)

Minimum fc′ is 17 MPa; maximum fc′ is None.

34
New cards

Limits for fc′​ (Normal-weight concrete for special moment frames and special structural walls)

Minimum fc′ is 21 MPa; maximum fc′ is None.

35
New cards

Limits for fc′ (Lightweight concrete for special moment frames and special structural walls)

Minimum fc′​ is 21 MPa; maximum fc′​ is 35 MPa.

36
New cards

Modulus of Elasticity

Modulus of elasticity of concrete is the ratio of the normal stress to corresponding strain for compressive stresses below the proportional limit. Concrete has no clear-cut modulus of elasticity. Its value varies with different concrete strengths, concrete age, type of loading, and the characteristics and proportions of the cement and aggregates.

37
New cards

Formula for Modulus of Elasticity (Ec​) for values of wc​ between 1440 and 2560 kg/m³

Ec​=(wc^1.5)​ (0.043fc′)​​ (in MPa)

38
New cards

Formula for Modulus of Elasticity (Ec​) for normal weight concrete:

Ec ​= 4700 √fc' (in MPa)

39
New cards

Minimum Spacing of Reinforcement (NSCP 2015 Section 425.2)

For parallel non-prestressed reinforcement in a horizontal layer, clear spacing shall be at least the greatest of 50 mm, db, and 4/3 dagg.

40
New cards

Minimum Spacing of Reinforcement (NSCP 2015 Section 425.2)

For parallel non-prestressed reinforcement placed in two or more horizontal layers, reinforcement in upper layers shall be placed directly above reinforcement in the bottom layer with a clear spacing between layers of at least 25 mm.

41
New cards

Minimum Spacing of Reinforcement (NSCP 2015 Section 425.2)

For longitudinal reinforcement in columns, pedestal, struts, and boundary elements in walls, clear spacing between bars shall be at least the greatest of 40 mm, 1.5db, and 4/3 dagg.

42
New cards

Bundled Reinforcement for Non-prestressed Elements (NSCP 2015 Section 425.6.1)

Groups of reinforcing bars bundled in contact to act as a unit shall be limited to four in any one bundle.

43
New cards

Bundled Reinforcement for Non-prestressed Elements (NSCP 2015 Section 425.6.1)

Bundled bars shall be enclosed within transverse reinforcement. Bundled bars in compression members shall be enclosed by transverse reinforcement at least 12 mm ϕ in size.

44
New cards

Bundled Reinforcement for Non-prestressed Elements (NSCP 2015 Section 425.6.1)

Bars larger than 36 mm ϕ shall not be bundled in beams.

45
New cards

Bundled Reinforcement for Non-prestressed Elements (NSCP 2015 Section 425.6.1)

Individual bars within a bundle terminated within the span of flexural members shall terminate at different points with at least 40db stagger.

46
New cards

Bundled Reinforcement for Non-prestressed Elements (NSCP 2015 Section 425.6.1)

Development length for individual bars within a bundle, in tension or in compression, shall be that of individual bar, increased 20% for a three-bar bundle, and 33% for a four-bar bundle.

47
New cards

Bundled Reinforcement for Non-prestressed Elements (NSCP 2015 Section 425.6.1)

A unit of bundled bars shall be treated as a single bar with an area equivalent to that of the bundle and a centroid coinciding with that of the bundle. The diameter of the equivalent bar shall be used for db in (a) through (e):

48
New cards

Specified Concrete Cover for Cast-in-Place Non-Prestressed Concrete Members (NSCP 2015 Section 420.6.1.3)

For concrete cast against and permanently in contact with ground, the specified cover for all members and reinforcement is 75 mm.

49
New cards

Specified Concrete Cover for Cast-in-Place Non-Prestressed Concrete Members (NSCP 2015 Section 420.6.1.3)

For concrete exposed to weather or in contact with ground, the specified cover for all members is 50 mm for 20 mm ϕ through 58 mm ϕ bars, and 40 mm for 16 mm ϕ bar, MW200 or MD200 wire, and smaller.

50
New cards

Specified Concrete Cover for Cast-in-Place Non-Prestressed Concrete Members (NSCP 2015 Section 420.6.1.3)

For concrete not exposed to weather or in contact with ground, the specified cover is 40 mm for 40 mm ϕ and 58 mm ϕ bars in slabs, joists, and walls; 20 mm for 36 mm ϕ bar and smaller in slabs, joists, and walls; and 40 mm for primary reinforcement, stirrups, ties, spirals, and hoops in beams, columns, pedestals, and tension ties.

51
New cards

Specified Concrete Cover for Bundled Bars (NSCP 2015 Section 420.6.1.3.4)

For bundled bars, specified concrete cover shall be at least the smaller of (a) and (b): a. The equivalent diameter of the bundle; b. 50 mm and for concrete cast against and permanently in contact with ground, the specified cover shall be 75 mm.

52
New cards

Strength Reduction Factors, ϕ (Table 421.2.1)

For moment, axial force, or combined moment and axial force (a): 0.65 to 0.90 in accordance with Section 421.2.2. Exception: Near ends of pretensioned members where strands are not fully developed, ϕ shall be in accordance with Section 421.2.3.

53
New cards

Strength Reduction Factors, ϕ (Table 421.2.1)

For shear (b): 0.75. Exception: Additional requirements are given in Section 421.2.4 for structures designed to resist earthquake effects.

54
New cards

Strength Reduction Factors, ϕ (Table 421.2.1)

For torsion (c): 0.75.

55
New cards

Strength Reduction Factors, ϕ (Table 421.2.1)

For bearing (d): 0.65.

56
New cards

Dead Loads

loads of constant magnitude that remain in one position. They include the weight of the structure under consideration as well as any fixtures that are permanently attached to it. For reinforced concrete building, some dead loads are frames, walls, floors, ceilings, stairways, roofs, and plumbing. Unit weight of concrete = 23.54 kN/m³.

57
New cards

Live Loads

loads that can change in magnitude and position. They include occupancy loads, warehouse materials, construction loads, overhead service cranes, equipment operating loads, and many others. In general, they are induced by gravity.

58
New cards

Environmental Loads

loads caused by the environment where the structure is located. For buildings, they are caused by rain, wind, temperature change, and earthquake. In fact, environmental loads are also live loads. Although they do vary with time, they are also caused by gravity or operating conditions, as is typical with other live loads.