1/22
Comprehensive vocabulary flashcards covering raw steel classifications, structural designations, mechanical stress-strain characteristics, manufacturing processes, and environmental degradation mechanisms from CENG 3334.
Mild Steel
A low-carbon steel containing less than 0.3% carbon, characterized by a balance between ductility and strength, lack of sensitivity to alloying metals, and common application in low-grade structural steels.
Medium Carbon Steel
Steel containing between 0.3% and 0.7% carbon that is sensitive to impurities and exhibits decreasing weldability as carbon content rises; includes standard structural steels such as A36, A572, and A992.
ASTM A36
A structural carbon steel with a minimum yield point of 36ksi (250MPa), a tensile strength of 58–80ksi (400–550MPa), a maximum carbon content of 0.26%, and standard availability across all plates, shapes, and bars.
ASTM A572
A high-strength low-alloy structural steel available in Grades 42, 50, 60, and 65 (corresponding to minimum yield points from 42ksi to 65ksi), commonly used for structural shapes, sheet piling, and tees.
ASTM A514
A high-yield-strength quenched and tempered alloy steel plate with a minimum yield strength of 90–110ksi (290–690MPa) and tensile strength of 100–130ksi (690–895MPa).
ASTM A588
A high-strength low-alloy structural steel with a 50ksi (345MPa) minimum yield point that provides atmospheric corrosion resistance, available in shapes, plates, and bars.
Bloom
A semi-finished rectangular or square raw steel product defined by a cross-sectional area A>36in2.
Billet
A semi-finished raw steel product typically having square cross-sectional dimensions ranging from 4 to 6inches.

Slab
A semi-finished raw steel product characterized by a rectangular cross section where the width is much greater than the thickness.
Structural Steel Shapes
Standard hot-rolled cross-sectional geometries used in civil construction, including Wide Flange (W Shape), American Standard Beams (S Shape), Angles (Equal and Unequal Legs), Channels (C and MC Shapes), Bearing Piles (HP Shape), Structural Tees (T Shape), Z Shapes, and Structural Tubing.

Continuous Casting
A modern steel manufacturing method where molten steel flows from a ladle into a tundish and mold, solidifies through a vertical cooling chamber, is guided and straightened through cool rollers, and is cut directly into blooms, billets, or slabs.

Elastic Region
The initial zone of a stress-strain curve where the material response is linear, small strain occurs proportionally to stress (σ=Eε), and all deformations are completely reversible upon unloading.
Yield Stress (Fy)
The stress level defining the transition from linear elastic behavior into the plastic region, characterized by significant permanent elongation occurring with little or no additional applied stress.
Strain Hardening
The stage of plastic deformation occurring after yielding where an increase in stress is required to induce further elongation until reaching the ultimate tensile strength.
Tensile Strength (Fu)
The peak engineering stress sustained by a steel specimen on its stress-strain curve, beyond which necking develops and structural failure/fracture follows.
Cold Drawn Steel
Steel that has been formed mechanically at temperatures below its transformational temperature, yielding elevated tensile strength at the expense of ductility.
Hot Worked Steel
Steel processed mechanically at temperatures above its recrystallization temperature, producing higher ductility with comparatively lower strength.
Modulus of Elasticity (E)
The slope of the linear elastic region relating stress to strain in structural steel, approximately equal to 29,000ksi (200GPa) at room temperature (70∘F).
Unit Weight of Steel
The nominal density of structural steel used in civil engineering design, equal to 490pcf.
0.2% Offset Method
A standardized graphical approach for establishing the yield point in materials lacking a distinct yield plateau by constructing a line parallel to the initial linear modulus beginning at a strain of 0.002 (0.2%).

High-Temperature Degradation of Steel
The property changes caused by elevated temperatures (such as 900∘F), resulting in decreased yield and ultimate strengths, decreased stiffness (E dropping to 25,000ksi), and increased ductility.
Pitting
An aggressive, localized form of corrosion that leads to the creation of deep holes, cavities, or perforations through steel elements.

Steel Section Loss
The physical reduction in cross-sectional steel thickness and bearing area resulting from extreme heat exposure or chronic corrosion.