1/17
Looks like no tags are added yet.
pure metals
solidify at single temperature
grains grow in direction opposite of heat transfer (columner grains)
alloys
solidification when temp drops below liquidus line
2-phase region, alloy is mushy or pasty and has columner dendrites
columner dendrites
tree-like solid arms in 2-phase region, arms grow until they interlock and no more liquid is left
slow cooling rates
coarse dendrites with large spacing between arms
fast cooling
fine structures, less spacing between dendrite arms
amorphous material (metallic glass)
caused by extremely fast cooling, no repeating pattern
microsegregation
under normal cooling rates, cored dendrites form from non-equilibrium cooling, composition at surface is different than center
macrosegregation
normal, inverse, gravity
normal segregation
non-equilibrium cooling, planar solidification front, low melting material to center
inverse segregation
non-equilibrium cooling, dendritic solidification front, low melting material to surface
gravity segregation
differing density of materials, heavy elements skink, lighter elements float
fluidity
capability of liquid metal to fill mold cavities
controlled by characteristics of molten metal (dependent) and casting parameters (independent)
why would you not heat a mold for better casting parameters to affect fluidity?
risk of expanding cavities and taking longer to cool
macroporosity
shrinkage and gasses
microporosity
dendrites
shrinkage fix
chilled surface, superheat, vented risers
gasses fix
flush with inert gas or pour in vacuum
dendrite fix
vibrating or increasing convection (directional grain growth)