1
New cards

8347) A primary reason why ordinary or otherwise nonapproved cleaning compounds should not be used when washing aircraft is because their use can result in A) hydrogen embrittlement in metal structures. B) hydrogen embrittlement in nonmetallic materials. C) a general inability to remove compound residues.

A) hydrogen embrittlement in metal structures.

2
New cards

8348) How may magnesium engine parts be cleaned? A) Soak in a 20 percent caustic soda solution. B) Spray with methyl ethyl ketone (MEK). C) Wash with a commercial solvent, decarbonize, and scrape or grit blast.

C) Wash with a commercial solvent, decarbonize, and scrape or grit blast.

3
New cards

8352) Which of the following are acceptable to use when utilizing chemical cleaning agents on aircraft? A) Cotton fiber wiping cloths when using a flammable agent and atomizing spray equipment. B) Microfiber wiping cloths when using a flammable agent and atomizing spray equipment. C) Synthetic fiber wiping cloths when using a flammable agent.

A) Cotton fiber wiping cloths when using a flammable agent and atomizing spray equipment.

4
New cards

8353) Select the solvent used to clean acrylics and rubber. A) Aliphatic naphtha. B) Methyl ethyl ketone. C) Aromatic naphtha.

A) Aliphatic naphtha.

5
New cards

8362) Which of the following are acceptable to use in cleaning anodized surfaces? A) Steel wool, aluminum wool, and fiber bristle brushes. B) Brass wire brushes and stainless steel wire brushes. C) Aluminum wool and fiber bristle brushes.

C) Aluminum wool and fiber bristle brushes.

6
New cards

8368) Which of the following is an acceptable first step procedure to help prevent scratching when cleaning a transparent plastic surface? A) Gently wipe the surface with a clean, dry, soft cloth. B) Flush the surface with clean water. C) Gently wipe the surface with a clean, soft cloth moistened with de-mineralized or distilled water.

B) Flush the surface with clean water.

7
New cards

8359) Which of the listed conditions is NOT one of the requirements for corrosion to occur? A) The presence of an electrolyte. B) Electrical contact between an anodic area and a cathodic area. C) The presence of a passive oxide film.

C) The presence of a passive oxide film.

8
New cards

8369) What should be done to prevent rapid deterioration when oil or grease come in contact with a tire? A) Wipe the tire thoroughly with a dry cloth, and then rinse with clean water. B) Wipe the tire with a dry cloth followed by a wash-down and rinse with soap and water. C) Wipe the tire with a cloth dampened with aromatic naphtha and then wipe dry with a clean cloth.

B) Wipe the tire with a dry cloth followed by a wash-down and rinse with soap and water.

9
New cards

8355) Caustic cleaning products used on aluminum structures have the effect of producing A) passive oxidation. B) improved corrosion resistance. C) corrosion.

C) corrosion.

10
New cards

8357) The rust or corrosion that occurs with most metals is the result of A) a tendency for them to return to their natural state. B) blocking the flow of electrons in homogenous metals, or between dissimilar metals. C) electron flow in or between metals from cathodic to anodic areas.

A) a tendency for them to return to their natural state.

11
New cards

8370) Galvanic corrosion is likely to be most rapid and severe when A) the surface area of the cathodic metal is smaller than surface area of the anodic metal. B) the surface areas of the anodic and cathodic metals are approximately the same. C) the surface area of the anodic metal is smaller than the surface area of the cathodic metal.

C) the surface area of the anodic metal is smaller than the surface area of the cathodic metal.

12
New cards

8371) Corrosion caused by galvanic action is the result of A) excessive anodization. B) contact between two unlike metals. C) excessive etching.

B) contact between two unlike metals.

13
New cards

8377) Which of the following statements is true? A) In the corrosion process, it is the cathodic area or dissimilar cathodic material that corrodes. B) In the Galvanic or Electro-Chemical Series for metals, the most anodic metals are those that will give up electrons most easily. C) In the Galvanic or Electro-Chemical Series for metals, the most cathodic metals are those that will give up electrons most easily.

B) In the Galvanic or Electro-Chemical Series for metals, the most anodic metals are those that will give up electrons most easily.

14
New cards

8372) Which of these materials is the most anodic? A) Cadmium. B) 7075-T6 aluminum alloy. C) Magnesium.

C) Magnesium.

15
New cards

8374) Which of these materials is the most cathodic? A) Zinc. B) 2024 aluminum alloy. C) Stainless steel.

C) Stainless steel.

16
New cards

8375) Of the following, when and/or where is galvanic corrosion most likely to occur? A) When an electrolyte (water) covers the surface of an aluminum skin, seeps into the cracks between lap joints, and oxygen is excluded from the area. B) At the interface of a steel fastener and aluminum alloy inspection plate in the presence of an electrolyte. C) In an area unprotected metal exposed to an atmosphere containing battery fumes, exhaust gases, or industrial contaminants.

B) At the interface of a steel fastener and aluminum alloy inspection plate in the presence of an electrolyte.

17
New cards

8354) Fayed surfaces cause concern in chemical cleaning because of the danger of A) forming passive oxides. B) entrapping corrosive materials. C) corrosion by imbedded iron oxide.

B) entrapping corrosive materials.

18
New cards

8356) Fretting corrosion is most likely to occur A) when two surfaces fit tightly together but can move relative to one another. B) only when two dissimilar metals are in contact. C) when two surfaces fit loosely together and can move relative to one another.

A) when two surfaces fit tightly together but can move relative to one another.

19
New cards

8358) Which of the following are the desired effects of using Alodine® (also known as Bonderite®) on aluminum alloy? A) A smooth painting surface and increased corrosion resistance. B) Relieved surface stresses. C) A slightly rough surface and increased corrosion resistance.

C) A slightly rough surface and increased corrosion resistance.

20
New cards

8378) Spilled mercury on aluminum A) greatly increases susceptibility to hydrogen embrittlement. B) may cause impaired corrosion resistance if left in prolonged contact. C) causes rapid and severe corrosion that is very difficult to control.

C) causes rapid and severe corrosion that is very difficult to control.

21
New cards

8349-1) For which of the following reasons would a water break test be conducted? A) To make certain that a newly alodized aluminum surface is sufficiently coated. B) To make certain that a bare metal surface is thoroughly clean. C) To make certain that an anodizing coating has been sufficiently removed before an electrical bonding connection can be made.

B) To make certain that a bare metal surface is thoroughly clean.

22
New cards

8360) The lifting or flaking of the metal at the surface due to delamination of grain boundaries caused by the pressure of corrosion residual product is called A) brinelling. B) granulation. C) exfoliation.

C) exfoliation.

23
New cards

8366) Corrosion should be removed from magnesium parts with a A) stiff, nonmetallic brush. B) silicon carbide brush. C) carborundum abrasive.

A) stiff, nonmetallic brush.

24
New cards

8363) Intergranular corrosion in aluminum alloy parts A) may be detected by surface pitting and white, powdery deposit formed on the surface of the metal. B) commonly appears as threadlike filaments of corrosion products under a dense film of paint. C) cannot always be detected by surface indications.

C) cannot always be detected by surface indications.

25
New cards

8363-1) Which of the following may not be detectable even by careful visual inspection of the surface of aluminum alloy parts or structures? A) Filiform corrosion. B) Intergranular corrosion. C) Uniform etch corrosion.

B) Intergranular corrosion.

26
New cards

8364) What may be used to remove corrosion from highly stressed steel surfaces? A) Steel wire brushes. B) Fine-grit aluminum oxide. C) Medium-grit carborundum paper.

B) Fine-grit aluminum oxide.

27
New cards

8349) When an anodized surface coating is damaged in service, it can be partially restored by A) applying a thin coat of zinc chromate primer. B) chemical surface treatment. C) use of a suitable mild cleaner.

B) chemical surface treatment.

28
New cards

8365) A primary cause of intergranular corrosion is A) improper heat treatment. B) dissimilar metal contact. C) improper application of primer.

A) improper heat treatment.

29
New cards

8361) A nonelectrolytic chemical treatment for aluminum alloys to increase corrosion resistance and paint-bonding qualities is called A) anodizing. B) alodizing. C) dichromating.

B) alodizing.

30
New cards

8376) One way of obtaining increased resistance to corrosion cracking is by A) relieving compressive stresses (via heat treatment) on the metal surface. B) creating compressive stresses (via shot peening) on the metal surface. C) producing nonuniform deformation while cold working during the manufacturing process.

B) creating compressive stresses (via shot peening) on the metal surface.

31
New cards

8367) Why is it important not to rotate the crankshaft after the corrosion preventive mixture has been put into the cylinders on engines prepared for storage? A) Fuel may be drawn into one or more cylinders and dilute or wash off the corrosion preventive mixture. B) The seal of corrosion preventive mixture will be broken. C) Engine damage can occur from hydraulic lock.

B) The seal of corrosion preventive mixture will be broken.

32
New cards

8373) The interior surface of sealed structural steel tubing would be best protected against corrosion by which of the following? A) Charging the tubing with dry nitrogen prior to sealing. B) Evacuating moisture from the tubing before sealing. C) A coating of linseed oil.

C) A coating of linseed oil.

33
New cards

8350) Select the solvent recommended for wipedown of cleaned surfaces just before painting. A) Aliphatic naphtha. B) Dry-cleaning solvent. C) Aromatic naphtha.

A) Aliphatic naphtha.

34
New cards

8351) Nickel-cadmium battery cases and drain surfaces which have been affected by electrolyte should be neutralized with a solution of A) boric acid. B) sodium bicarbonate. C) potassium hydroxide.

A) boric acid.

35
New cards

8026-1) If registration numbers are to be applied to an aircraft with a letter height of 12 inches, what is the minimum space required for the registration mark N1683C? A) 52 inches. B) 48 inches. C) 57 inches.

A) 52 inches.

36
New cards

8599) If masking tape is applied to an aircraft, such as for trim spraying, and is left on for several days and/or exposed to heat, it is likely that the tape will A) not seal out the finishing material if the delay or heating occurs before spraying. B) be weakened in its ability to adhere to the surface. C) cure to the finish and be very difficult to remove.

C) cure to the finish and be very difficult to remove.

37
New cards

8600) What is used to slow the drying time of some finishes and to prevent blush? A) Reducer. B) Retarder. C) Rubberizer.

B) Retarder.

38
New cards

8601) Which type of coating typically includes phosphoric acid as one of its components at the time of application? A) Wash primer. B) Epoxy primer. C) Zinc chromate primer.

A) Wash primer.

39
New cards

8602) Which properly applied finish topcoat is the most durable and chemical resistant? A) Synthetic enamel. B) Acrylic lacquer. C) Polyurethane.

C) Polyurethane.

40
New cards

8603) Aluminum pigment in dope is used primarily to A) provide a silver color. B) aid in sealing out moisture from the fabric. C) reflect ultraviolet from the fabric.

C) reflect ultraviolet from the fabric.

41
New cards

8604) A correct use for acetone is to A) thin zinc chromate primer. B) remove grease from fabric. C) thin dope.

B) remove grease from fabric.

42
New cards

8605) Which of the following is a hazard associated with sanding on fabric covered surfaces during the finishing process? A) Overheating of the fabric/finish, especially with the use of power tools. B) Static electricity buildup. C) Embedding of particles in the finish.

B) Static electricity buildup.

43
New cards

8606) When the humidity is low, what is likely to occur if unhydrated wash primer is applied to unpainted aluminum and then, about 30 to 40 minutes later, a finish topcoat is applied? A) Corrosion. B) A glossy, blush-free finish. C) A dull finish due to the topcoat "sinking in" to primer that is still too soft.

A) Corrosion.

44
New cards

8607) Fungicidal dopes are used in aircraft finishing as the A) first, full-bodied, brushed-on coat to prevent fungus damage. B) first coat to prevent fabric rotting and are applied thin enough to saturate the fabric. C) final, full-bodied, brushed-on coat to reduce blushing.

B) first coat to prevent fabric rotting and are applied thin enough to saturate the fabric.

45
New cards

8608) Before applying a protective coating to any unpainted clean aluminum, the aviation mechanic should A) wipe the surface with methyl ethyl ketone (MEK). B) remove any contaminants from the surface with a paper towel. C) avoid touching the surface with bare hands.

C) avoid touching the surface with bare hands.

46
New cards

8609) When humidity is low, what is likely to occur if hydrated wash primer is applied to unpainted aluminum and then, about 30 to 40 minutes later, a finish top coat is applied? A) Corrosion. B) A glossy, blush-free finish. C) A dull finish due to the topcoat "sinking in" to primer that is still too soft.

B) A glossy, blush-free finish.

47
New cards

8610) What is the usual cause of runs and sags in aircraft finishes? A) Too much material applied in one coat. B) Material is being applied too fast. C) Low atmospheric humidity.

A) Too much material applied in one coat.

48
New cards

8611) Which defect in aircraft finishes may be caused by adverse humidity, drafts, or sudden changes in temperature? A) Orange peel. B) Blushing. C) Pinholes.

B) Blushing.

49
New cards

8612) Which statement is true regarding paint system compatibility? A) Old-type zinc chromate primer may not be used directly for touchup of bare metal surfaces. B) Acrylic nitrocellulose lacquers may be used over old nitrocellulose finishes. C) Old wash primer coats may be overcoated directly with epoxy finishes.

C) Old wash primer coats may be overcoated directly with epoxy finishe