Pt 2. Chapter 5. "Fundamental Concepts of Enamel and Dentin Adhesion"

0.0(0)
Studied by 0 people
call kaiCall Kai
learnLearn
examPractice Test
spaced repetitionSpaced Repetition
heart puzzleMatch
flashcardsFlashcards
GameKnowt Play
Card Sorting

1/120

encourage image

There's no tags or description

Looks like no tags are added yet.

121 Terms

1
New cards

Q: What role does the smear layer play in dentin bonding?

A: It acts as a diffusion barrier decreasing dentin permeability, but is considered an obstacle that must be removed or modified to permit resin bonding.

2
New cards

Q: What major change led to the introduction of early dentin adhesives?

A: The idea that the smear layer should be removed via acid etching to improve in-vitro bond strengths.

3
New cards

Q: What technique was originally called "total-etch"?

A: Simultaneous acid application to enamel and dentin, now called the etch-and-rinse technique.

4
New cards

Q: How deep can dentin be demineralized by acids?

A: Up to ~7.5 µm depending on acid type, concentration, and application time.

5
New cards

Q: Why didn't early etched dentin show improved bond strengths?

A: The phosphonated resin was hydrophobic and did not bond well despite tubule penetration.

6
New cards

Q: What are examples of three-step etch-and-rinse adhesives?

A: All-Bond 2, All-Bond 3, OptiBond FL, Scotchbond Multi-Purpose.

7
New cards

Q: What are the three components of a three-step etch-and-rinse system?

A: (1) Phosphoric acid, (2) hydrophilic primer, (3) hydrophobic nonsolvated bonding resin.

8
New cards

Q: How does phosphoric acid affect dentin surface energy?

A: It removes high-energy hydroxyapatite and exposes low-energy collagen, decreasing surface-free energy.

9
New cards

Q: What is the purpose of the primer in a three-step system?

A: To increase dentin's critical surface tension, improving adhesive spreading and shear bond strength.

10
New cards

Q: What forms when primer and adhesive infiltrate etched dentin?

A: A hybrid layer and resin tags.

11
New cards

Q: What characterizes the hybrid layer in etch-and-rinse systems?

A: An abrupt transition between hybridized dentin and unaffected dentin with no visible gap.

12
New cards

Q: What drives the development of two-step etch-and-rinse systems?

A: Efforts to simplify the bonding protocol.

13
New cards

Q: Do two-step etch-and-rinse adhesives require a separate etch?

A: Yes.

14
New cards

Q: How do bond strengths of two-step systems compare to enamel bonding?

A: They approach enamel bond strength but still underperform compared to three-step systems.

15
New cards

Q: Give examples of two-step etch-and-rinse adhesives.

A: One-Step Plus, Prime & Bond NT, Adper Single Bond Plus, OptiBond SOLO Plus, PQ1, ExciTE F.

16
New cards

Q: What is missing from two-step etch-and-rinse systems compared to three-step?

A: A separate hydrophobic bonding resin layer.

17
New cards

Q: Why do two-step systems show more hydrolytic degradation?

A: Because hydrophilic primer components are mixed with hydrophobic monomers, making the layer more water-sensitive.

18
New cards

Q: What application technique improves their performance?

A: Active rubbing and multiple coats.

19
New cards

Q: Where were self-etch adhesives introduced?

A: Japan.

20
New cards

Q: What do the acidic primers in SEAs contain?

A: Phosphonated/carboxylated resin monomers that simultaneously etch and prime.

21
New cards

Q: Do SEAs require rinsing?

A: No.

22
New cards

Q: What advantage does simultaneous etching and infiltration provide?

A: Reduces risk of overwetting or overdrying dentin.

23
New cards

Q: What is a drawback of SEAs regarding enamel?

A: They etch enamel less effectively than phosphoric acid, especially uninstrumented enamel.

24
New cards

Q: What clinical issue has been linked to older SEAs at enamel margins?

A: Marginal discoloration and microleakage after long-term fatigue.

25
New cards

Q: Examples of two-step SEAs?

A: AdheSE, All-Bond SE, Clearfil SE Bond, Clearfil SE Bond 2, Clearfil SE Protect, OptiBond XTR.

26
New cards

Q: What is the pH of Clearfil SE Primer?

A: 1.9-2.0 (classified as a mild SEA).

27
New cards

Q: How are SEAs classified by pH?

A: Mild, moderate, aggressive.

28
New cards

Q: What is the clinical effect of selective enamel etching when using Clearfil SE Bond?

A: Improved marginal adaptation and less marginal discoloration.

29
New cards

Q: What molecule in Clearfil SE Bond allows chemical bonding to hydroxyapatite?

A: 10-MDP (creating nanolayering).

30
New cards

Q: Are SEAs less technique-sensitive than etch-and-rinse?

A: Yes.

31
New cards

Q: Do SEAs remove the smear layer completely?

A: No, smear remnants may remain and can affect bond strength.

32
New cards

Q: What steps are combined in one-step SEAs?

A: Etching, priming, and bonding in one solution.

33
New cards

Q: What problem arises when their acidic monomers contact self-cured composites?

A: Chemical incompatibility.

34
New cards

Q: Why do one-step SEAs undergo hydrolytic degradation?

A: They behave as semipermeable membranes and contain highly hydrophilic monomers.

35
New cards

Q: Examples of one-step SEAs?

A: AdheSE One F, Clearfil S3 Bond Plus, Bond Force, iBOND Self-Etch, OptiBond All-in-One, Xeno IV.

36
New cards

Q: What technique improves their performance?

A: Applying multiple coats and adding an extra hydrophobic layer.

37
New cards

Q: What was the retention rate of iBond at 18 months?

A: 40%; increased to 83.3% when a hydrophobic layer was added.

38
New cards

Q: What is a sign of incomplete sealing in simplified SEAs?

A: Transudation of dentinal fluid forming droplets on polymerized adhesive surfaces.

39
New cards

Q: What bonding strategies can universal adhesives be used with?

A: Self-etch, etch-and-rinse, and selective-etch.

40
New cards

Q: What do universal adhesives have in common with one-step SEAs?

A: They are one-bottle systems and benefit from an added hydrophobic resin layer.

41
New cards

Q: What major monomer do most universal adhesives contain?

A: 10-MDP.

42
New cards

Q: What is the bonding advantage of 10-MDP?

A: Ionic bonding to hydroxyapatite via nanolayering, forming stable MDP-Ca salts.

43
New cards

Q: What reduces the bonding ability of 10-MDP?

A: Presence of HEMA, which interferes with MDP-Ca salt formation.

44
New cards

Q: Why does active rubbing improve performance of universal adhesives?

A: Increases nanolayering, improves solvent evaporation, raises bond strength.

45
New cards

Q: Why does dentin show more nanolayering than enamel?

A: Dentin has more and smaller hydroxyapatite crystals oriented in criss-cross patterns, making it more receptive to MDP bonding.

46
New cards

Q: Do universal adhesives degrade over time?

A: Yes, show bonding degradation after 12-month water storage, similar to one-step SEAs.

47
New cards

Q: Why is drying dentin completely difficult clinically?

A: Because vital dentin is inherently wet.

48
New cards

Q: Why was research focused on adhesives compatible with humid environments?

A: Water was considered an obstacle to resin adhesion, prompting development of dentin adhesives suited for moist surfaces.

49
New cards

Q: What problem does the moist bonding technique prevent?

A: Collagen collapse in demineralized dentin, which would block monomer penetration into nanochannels.

50
New cards

Q: What solvents allow etch-and-rinse adhesives to work on moist dentin?

A: Acetone and ethanol.

51
New cards

Q: How do these solvents assist bonding?

A: They displace water from dentin and collagen, promoting monomer infiltration through collagen nanospaces.

52
New cards

Q: Why does moist bonding increase bond strength in vitro?

A: Water maintains collagen porosity, allowing better resin interdiffusion.

53
New cards

Q: Can excess water be removed without harming bond strength?

A: Yes, using damp cotton, suction, brushes, or tissue, without adverse effects.

54
New cards

Q: What happens if etched dentin is dried with air?

A: Collagen collapses and prevents resin monomer penetration, reducing bond strength.

55
New cards

Q: Which systems are more sensitive to overdrying?

A: Acetone-based adhesives (most), ethanol-based (less).

56
New cards

Q: What is the preferred appearance of etched dentin for bonding?

A: A glistening hydrated surface, not pooled with water.

57
New cards

Q: What structural change occurs when water is removed from collagen?

A: Loss of extrafibrillar water causes collagen to compact, reducing interfibrillar spaces.

58
New cards

Q: How much can the collagen network shrink when dried?

A: To one-third of its hydrated volume.

59
New cards

Q: What is seen under SEM/TEM when dentin is overdried?

A: Adhesive fails to penetrate; collagen fibrils coalesce without distinct interfibrillar spaces.

60
New cards

Q: Can dried demineralized dentin reexpand?

A: Yes, rewetting with water restores porosity and collagen's hydrated dimensions.

61
New cards

Q: Why does rehydration restore structure?

A: Water refills interfibrillar spaces, and collagen expands due to its intrinsic ability to rehydrate.

62
New cards

Q: Is rewetting dentin after checking for "frosty enamel appearance" acceptable?

A: Yes, rewetting is acceptable clinically.

63
New cards

Q: Why is pooled moisture undesirable?

A: It dilutes primer and reduces effectiveness.

64
New cards

Q: Why is active rubbing of primer/adhesive beneficial?

A: It improves infiltration, aids water evaporation, and reduces nanoleakage.

65
New cards

Q: What clinical evidence supports vigorous rubbing?

A: Prime & Bond NT showed 92.5% retention with vigorous rubbing vs. 82.5% without it at 24 months.

66
New cards

Q: Why may moist dentin not be necessary for universal adhesives used etch-and-rinse?

A: They contain 10-20% water, which can rehydrate dried dentin.

67
New cards

Q: How do bond strengths compare on moist vs. 10-second air-dried dentin with universal adhesives?

A: They are similar.

68
New cards

Q: Why does leaving dentin moist reduce bond strength with universal adhesives?

A: Residual water after air-drying increases hydrolytic degradation and lowers bond strength.

69
New cards

Q: What is ethanol wet-bonding?

A: Replacing water in etched dentin with 100% ethanol before bonding.

70
New cards

Q: What effect does ethanol wet-bonding have on bond strengths?

A: It significantly increases bond strengths of both hydrophobic and hydrophilic resins.

71
New cards

Q: Why is ethanol wet-bonding not clinically adopted yet?

A: It requires an extra step, is time-consuming, and lacks clinical evidence.

72
New cards

Q: What is the primary cause of adverse pulpal reactions after restorative procedures?

A: Bacteria remaining in, or penetrating, the preparation, not the restorative material itself.

73
New cards

Q: Can adverse pulpal reactions result from multiple factors?

A: Yes, they are often caused by a combination of factors.

74
New cards

Q: How can bacterial invasion contribute to pulpal reactions?

A: It may invade from the tooth preparation or from an existing carious lesion. (Factor 1)

75
New cards

Q: How can a faulty restoration cause pulpal problems?

A: It allows bacterial penetration into the pulp. (Factor 2)

76
New cards

Q: How can improper moisture control or cementation cause pulpal irritation?

A: Excessive desiccation or excessive pressure can create a harmful pressure gradient. (Factor 3)

77
New cards

Q: How can trauma cause pulpal reactions?

A: Through traumatic injuries to the tooth. (Factor 4)

78
New cards

Q: How can iatrogenic errors in tooth preparation cause pulpal damage?

A: Excessive pressure, heat, or friction during preparation. (Factor 5)

79
New cards

Q: How does composite polymerization temperature affect the pulp?

A: Pulpal temperature rise occurs during polymerization, especially with flowable composites. (Factor 6)

80
New cards

Q: What stress-related factor can damage the pulp?

A: Stress from polymerization contraction of composites and adhesives. (Factor 7)

81
New cards

Q: How can incomplete curing harm the pulp?

A: Unpolymerized resin monomers can cause adverse pulpal reactions. (Factor 8)

82
New cards

Q: Why are enamel peripheries important for biocompatibility?

A: Enamel margins allow strong adhesion that counters polymerization shrinkage stresses.

83
New cards

Q: How do enamel margins affect bacterial sealing?

A: Strong enamel adhesion reduces marginal gaps and helps seal the restoration against bacteria.

84
New cards

Q: What types of dentin have increased mineral content?

A: Aged dentin, dentin beneath carious lesions, and dentin exposed in NCCLs where tubules are obliterated by tricalcium phosphate.

85
New cards

Q: What is dentin that undergoes mineralization changes called?

A: Sclerotic dentin.

86
New cards

Q: How does sclerotic dentin respond to acid etching compared to normal dentin?

A: It is much more resistant to acid etching.

87
New cards

Q: How does sclerotic dentin affect adhesive penetration?

A: Penetration of dentin adhesive is limited.

88
New cards

Q: How do bond strengths to sclerotic dentin compare to normal dentin in NCCLs?

A: They are low for both etch-and-rinse and self-etch techniques.

89
New cards

Q: Is clinical effectiveness in sclerotic dentin lower than in normal dentin?

A: Yes, sclerotic cervical lesions show reduced effectiveness.

90
New cards

Q: Do some adhesives perform better in sclerotic dentin?

A: Yes, some specific adhesives may perform better in sclerotic dentin than in normal dentin.

91
New cards

Q: How might masticatory forces influence NCCLs?

A: They may contribute to their formation.

92
New cards

Q: How can bruxism or eccentric forces affect Class V restorations?

A: By generating lateral forces that cause cyclic fatigue and bond failure.

93
New cards

Q: Why are NCCLs often used as clinical tests for adhesives?

A: Because bonding to NCCLs is particularly challenging.

94
New cards

Q: What property influences composite shrinkage?

A: The inorganic filler load.

95
New cards

Q: Why do microfilled composites relieve stress better?

A: They have a low elastic (Young's) modulus, allowing flow during polymerization or tooth flexure.

96
New cards

Q: What happens with composites that have a high Young's modulus?

A: They cannot relieve stresses, transferring them to the adhesive interface, potentially causing debonding.

97
New cards

Q: Has improved adhesive strength reduced the significance of composite stiffness?

A: Yes, some clinical studies show no difference in Class V retention due to stiffness.

98
New cards

Q: Which materials showed the best clinical retention in NCCLs?

A: GIC-based materials.

99
New cards

Q: Which adhesive systems showed clinically reliable performance?

A: Three-step etch-and-rinse and two-step SEAs.

100
New cards

Q: Which adhesives performed poorly?

A: Two-step etch-and-rinse adhesives (less favorable) and one-step SEAs (worst).