1/27
Lecture 10
What is injection molding?
a manufacturing process where liquid plastic resin is pushed into a mold, cools and forms a plastic part
What are the pros of injection molding?
cost effective mass production
low material waste, rapid rate of production, highly automated
repeatable
precise
versatile material selection
high strength, flexibility, heat resistance, transparency
What are the cons to injection molding?
expensive tooling
non-agile design
almost all design changes require tool changes
some limitations to part geometry
uniform wall thickness
low wall thickness
undercuts are possible but add complexity and cost
What are the characteristics of thermoplastics?
can be melted and reformed repeatedly
usually come in bead or granular form
what are the characteristics of thermosets?
once cured, heat will not re-melt them
usually liquid at room temperature, part a and part b mixed during injection process
can be filled with non-organic material like carbon fiber, Teflon, glass beads
What are the three main subsystems in injection molding?
injection unit
clamping unit
mold
What does the injection unit do?
feeds, melts and fills mold cavity with liquid plastic material
what does the clamping unit do?
closes mold parts together, holds molds together while plastic sets, ejects the finished part
what does the mold do?
two primary plates that form the negative cavity of the part shape together - one stationary (front/A) and one moving (rear/B)
What are the different parts of the injection unit?
hopper
holds plastic pellets, is fed by an operator, opens into the barrel
barrel
outer case that houses screw and liquifying plastic
heaters
wrapped around the barrel, head the plastic inside to melting temperature
screw
driven by motor, acts as an auger to convey melting plastic from the hopper to the valve
tapered larger as it nears the distal end
rotates to convey plastic, translates to force plastic into mold
no-return valve
delivers plastic from barrel into the mold
prevents backflow of material
material delivered into mold is called a “shot”
What are the different parts of the clamping unit?
platens
the stationary platen holds the front half of the mold
the moveable plate moves the rear half of the mold by sliding along the tie bar
tie bar
supports moveable platen during translation
aligns mold halves
clamping system
moves the moveable platen
ejection system
How does the ejection system work?
“rides along” with moving platen while part is formed
when molds separate, ejection plate moved forward with respect to the moving platen, pushing plastic part out of the mold
What are the characteristics of molds?
attached to the platens on the clamping unit
have negative volume cavities that match the form of the part
mainly consist of two halves
can have cooling channels built into to aid in part solidification
includes special features like sprues, gates, and runners to manipulate the flow of liquid material
What are the process steps in injection molding?
two mold halves close together
plastic is injected into the mold
part dwells as temperature drops and material solidifies
mold halves separate
part is ejected
Which components belong to the injection unit?
Hopper, Ejection system, Barrel, Tie Bar, Screw/Auger, Integrated active cooling, Platens, Heaters, Valve
hopper
barrel
screw/auger
heaters
valve
Which components belong to the clamping unit?
Hopper, Ejection system, Barrel, Tie Bar, Screw/Auger, Integrated active cooling, Platens, Heaters, Valve
ejection system
tie bar
platens
Which components belong to the mold?
Hopper, Ejection system, Barrel, Tie Bar, Screw/Auger, Integrated active cooling, Platens, Heaters, Valve
integrated active cooling
Where does the ejection system reside in an injection molder?
moving platen
the ejection pin size, quantity, and configuration is part specific
true or false
true
What are some extra considerations for injection molding?
wall thickness
ribs
What features does draft affect injection molding?
wall thickness
surface texture
pocket depth
feature type
What is a rule of thumb for rounds and fillets in injection molding?
radii that determine wall thickness should attempt to maintain consistent wall thickness
fillets should be about ½ adjacent wall thickness
what is the rule of thumb for wall thickness?
should be uniform thickness
features that would concentrate “thermal mass” in a single area should be separated
what happens when walls are thick?
cause cosmetic and structural issues such as warping and voiding
what happens when walls are thin?
increase injection pressure
reduce structural strength
fail to fill at all
What causes thermal sink?
cooling time differential between thick and thin areas
how can thermal sink be prevented?
smoothing transition from thick to thin areas
managing thickness ratio between superficial and deep features