Endogeneous
Inward growth (palm trees)
Most commonly used tree growth type for building
Exogeneous
Exogeneous
Outward growth in rings
Deciduous
Broadleaf, hardwood
Coniferous
Cone bearing (evergreen), softwood
Deciduous examples
Oak, ash, maple, walnut
Coniferous examples
Douglas fir, pine, spruce, cedar
Spring ring growth
Light ring, fast with thin hollow walls
Summer ring growth
Dark ring, thick strong wall growth
Wider annual rings indicate:
Fast growth rate
Pith
Center stem
Heartwood
Second layer, provides structural support
Sapwood
Third layer, carries sap
Cambium
Fourth layer, growth area, very thin
Inner/outer bark
Outer layers of tree
Radial axis
Perpendicular to growth
Tangential axis
Parallel to growth, weakest
Longitudinal axis
Parallel to grain, strongest
Cellulose
50% of wood, a strand-forming polymer
Fibrils
Strands formed by cellulose
Wood fibers
Cell walls made up of fibrils
Lignin
“Glue” that binds tubes together
% of lignin in softwood?
23-33%
% of lignin in hardwood?
16-25%
Fiber Saturation Point
MC when wood cells are saturated but no free water exists
MC>FSP
Changes in MC only affect density and wet weight of wood
MC<FSP
Typical after mill, small changes lead to great effects in all properties of wood
Ratio of % shrinkage to % MC
1% shrinkage per 5% MC
Dimensional Lumber
Light framing: studs, joists, beams, rafters, trusses, decking. 2×4, 2×6
Heavy Timber
Heavy framing: railroad ties, landscaping. 4×6, 6×6, 8×8
Flat Sawing
Lowest quality, grain is <45 deg. from flat side of saw
Rift Sawing
Grain is 45-80 deg. from flat side of saw
Quarter/Edge Sawing
Highest quality, grain is 80-90 deg. from flat side of saw
Seasoning step of lumber production
Drying of wood
Uneven shrinkage
What part of the seasoning process can cause defects?
Method of seasoning wood
Combo of:
Air drying (cheap and slow)
Kiln drying (expensive and fast)
MC of wood after cut
30-200%
MC of wood after mill
15%
Surfacing step of lumber production
Planing, taking 1/4”+ from each side
What are the real dimensions of a 2×4 and why?
1.5×3.5, because the dimensions are based on the size before the surfacing step
A “dressed” piece of wood
Surfaced on all four sides
Causes of lumber defects
Natural growth, seasoning, disease, insects, faulty processing
Knot
Most common defect, the site of where a branch grew
Shake
Separation between annual rings
Wane
Weak bark or soft wood left on edge
Sap Streak
Line of sap left in wood
Pitch Pocket
Resin filled openings in rings
Check (Split)
Rupture across rings
Warping
Caused by uneven drying or shrinkage
Bowing
Curvature along the length
Crooking
Curvature along the face
Cupping
Edges roll up
Twisting
Corner lifts
Specific Gravity of cell walls
~1.5
Dry density of wood
~20-45 lb/ft³
Thermal Conductivity of wood
Better than metal, worse than insulation
Modulus of Elasticity of wood
~1×10^6 psi - 2×10^6 psi, depends on species, MC, SG, grain direction
Plywood
Panel made from plies glued together. Expensive, used structurally
Oriented Strand Board (OSB)
Panel, used for floors
I-Joist
Two 2×4s or 2×6s + an OSB web
Glue Laminated Beam (GLULAM)
Parallel grain glued together, used decoratively
Dead Load
Weight of the structure itself
Live Load
Occupants: furniture, people, removable items
PSF to PLF
Multiply the psf load by the tributary width
Tributary Width
Portion of floor supported by one beam: half of beam spacing on each side of the beam
Bending moment equation
M=((distributed load)*(span of beam)²)/8
Allowable bending stress
Found by table and adjusted by factors (fb,allow)
Actual bending stress
fb=Mc/I or M/S,
M is the bending moment
S is from the chosen beam size
Relationship between allowable and actual bending stress
Actual<allowable, this will determine the size of beam used
Mortar makeup
Water, aggregate, cement
Mortar uses
Goes inbetween units
bonds units
creates a bed layer and level surface
aesthetic
Grout makeup
High slump concrete, aggregate, water, cement
Grout uses
Goes inside units
bonds units
bonds reinforcements to units
fills voids in CMUs
increases bearing area
increases fire resistance and overturning resistance
Mortar types from strongest to weakest
M, S, N, O
Type M Mortar lime and sand makeup
¼ part lime, 3.5 parts sand
Type M Mortar properties
Brittle, strongest, used for reinforcement
Type S Mortar lime and sand makeup
½ part lime, 4.5 parts sand
Type S Mortar properties
Typical mortar
Type N Mortar lime and sand makeup
1 part lime, 6 parts sand
Type N Mortar properties
Typical mortar
Type O Mortar properties
Fluid, weakest
Type O Mortar lime and sand makeup
2 parts lime, 9 parts sand
CMU
Concrete masonry unit
Types of CMUs
Solid, hollow, light, medium, heavy, load bearing, non load bearing
Properties of lightweight CMU
Higher thermal and sound resistance
Solid CMU area
XS area>75% total area
Hollow CMU area
XS area<75% total area
Specified dimension
Size of unit
Nominal dimension
Size of unit + half of mortar joint on each side
Prism test
Tests bricks by stacking with mortar, placing in bag, curing, and compression+tensile strength testing
IRA
Initial rate of absorption, measures how quickly a brick removes water from mortar
Unit Strength test
Brick strength is calculated with tables, is usually a lower value than prism test results
Course
Horizonal layer of masonry units
Wythe
Vertical layers of courses (a 1 brick deep wall)
Stretcher
Normal brick position
Rowlock
Stretcher turned on its side (perpendicular to stretcher)
Header
Rowlock flipped onto the thicker side (head facing front)
Soldier
Standing brick (vertical stretcher)
Bed Joint
Horizontal layer where bricks are laid
Head joint
Vertical layer between bricks