1/20
what are some of the possible problems with an eccentric prestress and straight layout?
excessive hogging moment Pe is applied in sections not close to mid-span leading to risk of damage in transport
excessive cambers
excessive decompression in top fibre after transfer
what is full prestress?
assuming tension stresses are not allowable no matter how small they are
what is the critical condition to prevent decompression of top fibre (y=ytop)?

in full compression, what is the cable layout equal to?
the shape of the moment diagram and the deformed shape w/o prestress
how can strands be profiled in a pretensioned beam with a bent cable?
pinning them to the prestressing bed
why is pretensioning not always the best option for prestressing?
if the beam is longer or has a more complex loading situation then cable profiling is more difficult
in post-tensioned elements produced in-situ, what duct characteristic vary?
material depending on flexibility required, plastic or metallic
surface finish, smooth or corrugated
for in-situ post tensioning, what is the production process?
ducts are laid out
cast concrete
demould ducts
install cables into ducts
adequately position with jackbolts
install tendons, grips and jacks
tension grips and jacks
what are the different methods for post-tensioning?
bonded and unbonded
name and define the different unbonded methods of post-tensioning
external (deviated)
internal (tendons are embedded in concrete in all sections)
what is needed to ensure an adequate bonded tendon?
grouting (bonds stands to ducts)
corrugated ducts (bonds between tendons and concrete)
what is grease used for in unbonded tendons?
grease is used for corrosion protection, but allows relative displacement of strands
what is a key fact to remember in analysis of unbonded tendons?
there is no strain compatibility between concrete and tendons
give some examples of external unbonded tendons
precast segmental bridges with box-section segments
how are composite sections reflected in elastic equations?
using the parameters of a transformed section, concrete is the reference material for the transformation
how is axial stiffness of a composite section calculated?
axial stiffness = EcA*=EcAc + EsAs + EpAp
how is flexural stiffness of a composite section calculated?
flexural stiffness = EcI* = EcIc + EsIs + EpIp
what is the main principle when reflecting composite sections in elastic equations?
the stiffness parameters of the transformed section must accurately represent the stiffness of the real element
how are the moduli ratios determined?
rearranged the axial stiffness equation for A*:
A* = Ac + nsAs + npAp
where ns = np = 6.25
what are A* and I* equal to for bonded tendons?
A* = Ac + npAp
I* = Ic + npIp
Ip=Ape2
why are npAp and npIp equal to 0 for unbonded tendons?
with unbonded tendons there is no solidarity between them and other materials so there is no strain compatibility between them and the composite section