1/8
Looks like no tags are added yet.
solvus line
the locus of points on a phase diagram representing the limit of solid solubility as a function of temperature
resilience
The capacity of a material to absorb energy when it is elastically deformed.
proportional limit
The point on a stress-strain curve at which the straight-line proportionality between stress and strain ceases.
poisson’s ratio
For elastic deformation, the negative ratio of lateral and axial strains that result from an applied axial stress.
strain hardening
The increase in hardness and strength of a ductile metal as it is plastically deformed below its recrystallization temperature.
pearlite
A two-phase microstructure found in some steels and cast irons; it results from the transformation of austenite of eutectoid composition and consists of alternating layers (or lamellae) of a-ferrite and cementite.
T or F: Rapid cooling(quenching) is used to form martensite because it prevents carbon atoms from diffusing out of the crystal structure
T
Why is as-quenched martensitic steel almost always tempered before being used in engineering applications
it is extremely brittle and has high internal stresses
on a binary phase diagram, what does the solidus line represent
the temperature below which the alloy is completely solid