1/79
Looks like no tags are added yet.
structural steel use
plates, bars, pipes structural shapes etc
steel fastening products
bolts, buts, washers
reinforcing steel use
rebar for concrete
Steel production process
Reduction of iron ore to pig iron (high carbon)
blast furnace with carbon (coal +coke) and limestone
limestone removes impurties from iron ore
slag: molten rock + impurities skimmed off top
molten iron with carbon is collected at bottom
Refining pig iron to steel
remove excess carbon + other impurities by oxidation in furnace
Basic oxygen furnace- 300 tones in 25 mins
electric arc- melts steel (lots of energy)
Forming steel into products
cast into ingots (large blocks that must be remelted and reshaped)
continuous shapes (casting) - rolled shapes, plates, bars
Carbon in steel
higher carbon: steel is harder and more brittle
cast iron: high carbon (>2%) = brittle
Higher carbon steel: medium carbon (0.8-2%)= brittle
Structural steel: low carbon (0.15-0.27%) = ductile
Allotropic
different crystal structures at different temperatures
Crystalline
solid state, metal atoms arragned in orderly repeating 3D pattern
Crystal lattice structures
BCC: Body centered cubic
FCC: Face centered cubic
Molten steel structure
solidfies and forms crystals called grains
room temp: BCC fashion
high temp: FCC Structure, austentite
below transition temp: BCC
ferrite and pearlite
Pearlite
combination of ferrite and cemntite
Ferrite
low carbon (soft, ductile)
Cementite
high carbon (hard)
Heat Treatment
process of heating and cooling
changes physical and mechanical properties of steel
Austenite decomposition
one FCC lattice structure of steel
heating steel in this range and cooling it is known as Austenite decomposition
how decomposition is done (rate of cooling) key to heat treatment
Annealing
softening process carried out by heating above the austenitic temperature then slowly cooling to room temperature
steel gets softer and more ductile increasing toughness making it more workable
Hardening
higher heat (into austenitic range) then rapid cooling by quenching in water/ brine/ oil
rapid cooling changes grain structure into martensite (strong but brittle)
harder and more brittle requires tempering (heating to lower temp)
after quenching steel is cooled then reheated
Steel alloys
steel + alloying metal to change properties
hardenability
corrosion resistance
machineability
ductility
strength
5% of steel composition are elements other than iron
Structural Steel
hot rolled structural shapes, plates, and bars used in columns, beams, brackets, frames etc.
grades determined by mechanical properites (yield strength, ultimate strength, % elongation)
Types of structural steel used for structural application
low carbon (<0.3%)
medium carbon (0.3% - 0.6%)
Steel section shapes
Wide flange
I beam
Channel
Equal Leg angle
Unequal leg angle
Tee
Sheet piling
Rail
Conventional Reinforcing Steel
plain bars, deformed bars, and deformed wire fabrics
bars made from 4 steel types
A615 (billet)
A616 (rail)
A617 (axle)
A706 (low-allow0
Steel for pre-stressed concrete
requires special wires, strands, cables, and bars
must have high strength + low relaxation properties
higher ultimate strength than steel shapes
ASTM A416, grade 270 = ultimate strength 270 ksi
Tension test for steel
most important test
determines
yield strength, ultimate strength (tensile), elongation and reduction of area (poissons ratio)
plate, sheet, round rod, and tube can be treated
typical specimen: round or rectangular
Charpy vs Notch impact test
measures toughness or fracture energy at different temperatures
specimen of rectangular with a notch Charpy machine and pendulum that breaks it
Energy absorbed at a high temp is what? low temp?
high temp = high energy
shear = ductile
low temp = low energy
cleavage = brittle
Hardness test
measures resistance to small dents + scratches
Spring load indenter
forced into the surface of material with specified load and rate
depth or size is related to hardness number
What is required for corrosion?
Anode
cathode
conductor
electrolyte
Anode
positive electrode when corrosion occurs
Cathode
negative electrode needed for electrical current
Conductor
metallic pathway for e- to flow between electrodes
Electrolyte
liquid support flow of e-
moisture (in air)
Steel corrosion
Oxidation (steel): serious weakening of structures
Anode: ferrous ions go into solution
cause e- to be released from anode and move through steel to cathode
Cathode: e- combine with oxygen and water to form hydroxyl ions
react with ferrous ions to produce ferrous hydroxide
Corrosion Protection method
barrier coating: isolate steel from moisture
Inhibitive coatings: pigments migrate to surface to passivate the surface
cathodic protection: electrically connect to sacrificial metal (loses e’ before reached steel)
What are the types of asphalts used in pavements
asphalt cement (asphalt binder)
asphalt emulsion
used for cold mix applications
60-70% asphalt, 30-40% water
Asphalt cutback
solvents
used for cold mix applications
Asphalt Cement (binder) characteristics
Hot mix asphalt (HMA)
sticks the aggregates together
waterproof
fairly durable
resistant to reaction with most acids, salts etc
temperature sensitive
What are the asphalt pavement layers
Top: Surface course - wearing or finish layer
provide uniform and durable roadway
Base course
layer of pavement helping to distribute loads
Subbase
used if sub grade is of poor quality
crushed aggregate, compact gravels
Sub grade (base aka ground)
serves as the foundation
What properties does asphalt binder have
visco - elastic material
viscous at high temps (fluid)
elastic at low temps (solid)
depends on temp and loading rate
what is asphalt cement used to do
asphalt binder
used for sealing and waterproofing
Asphalt concrete
asphalt binder + aggregate
used mainly for hot mix asphalt pavement surfacing (HMA)
Soft vs hard grade of asphalt
Soft (low viscosity)
used in cold climates to avoid thermal cracking
Hard (high viscosity)
used in hot climates to avoid rutting
Penetration grading
obsolete
test:
measures consistency of binder using a weighted needle loaded for 5 secs
viscosity grading
AC
based on viscosity testing
tests:
shear deformation resistance of viscous mat
absolute - uses vacuum viscometers for different binders
60 degrees C
kinematic - no vacuum needed
tested at 135 degrees C
Aged residue grading
AR
viscosity of conditioned binders
Performance grading
PG (superpave)
focused on rutting fatigue and thermal cracking
intended to improvev pavement performance by reducing potential to:
permanent deformation
fatigue cracking
low temperature cracking
excessive aging from volatilization
pumping and handling
Testing associated with performance grade
flash point
viscosity (rotational)
dynamic shear rheometer
bending beam rheometer
direct tension
Rotational Viscometer
measures viscosity
ability to pump binder at asphalt plant
establish temp vs viscosity relationship
Dynamic Shear Rheometer
tests complex shear modulus of binders
measures the resistance to shear deformation
Bending Beam Rheometer
tests low temperature stiffness properties of binders
measures midpoint deflection of simply supported beam
Direct Tension
thermal cracking properities
Superpave aggregate gradation specs
specifies control points (on 0.45 power graph) that gradation must go through
Asphalt Cutbacks
asphalt cement +solvent
graded by curing time and viscosity
RC = rapid curing 5-10 mins
MC = medium curing = few days
SC = slow curing = a few months
Asphalt Emulsions
binder + water + emulsifier
Graded by setting time viscosity
RS = rapid setting 5-10 mins
MS = medium setting = several hours
SS = slow setting = a few months
Why is emulsion preferred over cutback
safer
used with damp aggregates
slightly more economic
better environmentally
Asphalt concrete (hot mix asphalt)
asphalt binder + aggregates
flexible pavement = 93% of 2 million miles of paved roads
Desirable properties for asphalt pavements
stable: resist permanent deformation under load
fatigue resistant: under repeating load
resistant to thermal cracking: due to contraction at low temps
resistant to hardening or aging: during production and in service
skid resistant: texturing surface
workable: ease of mixing, placing, compacting
Phase diagram
Mass - volume relationship
air
binder
aggregate
Rutting
accumulation of permanent deformation in the wheel path
Fatigue Cracking
repeated bending
Thermal Cracking
temperature gradient
Aging & oxidation
stiffening
Stripping
loss bond between binder and aggregate from moisture
Advantages of AC recycling
economy
energy
environment
eliminates problem of reconstruction
maintains bridge and tunnel clearances
Voids in total mix (VTM)
air voids embedded in the HMA
4% starting point in mix design
Voids in mineral aggregate (VMA)
measure of the asphalt film thickness
controls the minimum asphalt content
decreases as nominal max aggregate size increases
large agg have less surface area
Voids filled with asphalt (VFA)
percent of the VMA filled with asphalt
mix design controls the max asphalt content
Composite
two or more distinct materials or phases (reinforced concrete)
Yield Strength
stress level where steel ceases to behave elastically and where the ration of stress to strain decreases significantly
Ultimate Strength
the greatest stress a material can sustain before the material will fail by breaking
Microscopic composites
fibers or particles in sizes up to a few hundred microns
Macroscopic Composites
constituents of much larger size, such as aggregate particles and rebars in concrete
Phases of microscopic composites
Consist of:
continuous phase - polymer (plastic)
dispersed or reinforcing phase
Matrix Phase:
surrounds, suspends, and binds fibers or particles
transfer load to them
protects them against environmental attack and damage due to handling
Dispersed Phase: (fiber)
harder and stiffer than the matrix phase
Fiber reinforced polymers (FRP)
fibers dispersed in matrix as polymer
whiskers (very thin single crystals, high cost, poor bond)
Fibers (glass, carbon and graphite, boron, ceramic etc.)
stronger than bulk material (300x stronger)
FRP Composition
made from:
glass (most common)
carbon
aramid (kevlar)
from resins:
epoxies
vinyl esters
Matrix of FRP
used to:
bind fibers together
protects fibers
separates fibers
transfers forces to the fibers (shear stress)
Thermosetting resins characteristics
deteriorate at elevated temps
repeatedly heated without damage
As the percentage of carbon increases in steel we can expect what with the strength
higher strength
"Quenching" of steel refers to
rapid cooling
The standard way to "roll" steel today is through
continuous casting
In steel, percent elongation is a measure of what?
ductility