Integrating Cl2 EWC into VIP NMOS Process - Study Notes
Integrating Cl2 EWC into VIP NMOS Process
Objective & Overview
- Objective:
- Compare the impact of replacing the HCl EWC (Enhanced Wet Chemical) Process of Record (POR) with Cl2 EWC on the VIP proxy SiP process.
Test Plan Timeline & Procedures
- Key Items:
- Transfer VIP Proxy recipes to Chamber 51-6:
- Clean and main recipes; deadline: 07-31-2024.
- Baseline VIP Proxy process on 51-6 with HCl EWC:
- Set as reference; run 3x for sanity check; deadline: 07-31-2024.
- Replace HCl with Cl2 EWC (Ironman Version):
- Optimize thermal traces using Si wafers (without process via SemiAuto) and perform 3x sanity checks; deadline: 07-31-2024.
- Chamber Inspection:
- Detailed quartz and exhaust flange inspection with photos (no breaking vacuum); deadline: 08-02-2024.
- Repeatability Test:
- Run 25x with both HCl and Cl2 EWC; deadline: 08-14-2024.
- Recipe tuning:
- Tune Cl2 etching parameters (flow rate, temperature, time) for best Wafer-to-Wafer (WtW) performance; deadline: 08-21-2024.
- Final Repeatability test:
- Use full stack (SiAsP + SiP) including quartz and exhaust flange inspection; deadline: 08-28-2024.
- Share optimized Cl2 EWC process:
- Distribute recipe with changes in wafer loading and unloading temperature settings; deadline: 09-02-2024.
Process Requirements
- Maintaining Thermal Transitions:
- Cool down to Cl2 etch temperature.
- Keep quartz temperature high to enhance etch efficiency.
- Heat up quickly after etching for proper wafer processing continuation.
Main & Cl2 Recipe Steps
- Cl2 Recipe Steps:
- Start: 5s at 530°C.
- Carrier: 5s.
- Etch Fill: 15s.
- Hold: 10s.
- Restore: 15s.
- Purge: 10s.
Thermal Performance & Stability
- Thermal Traces documented at various temperature settings (e.g., 530-520°C, with stabilization time specifics).
- Optimize wafer load/unload conditions to enhance etching and simplify wafer transfers.
Weight Thickness Measurement (WtW) Check
- Comparison of Cl2 EWC with HCl EWC noted that both showed closely overlapped SiP thickness profiles, indicating minimal impact from new thermal settings.
Inspection Results & Chamber Conditions
- Inspection for both HCl and Cl2 EWC indicated closely matched thickness profiles and phosphorus concentration from materials used in processes.
- Chamber condition pre and post-marathon showed virtually no changes in chamber status.
Cl2 EWC Tuning Timeline
- Continuous process improvements with specific details for establishing and transitioning to Cl2 EWC, alongside key unchanged processes for the upcoming assessments.
Final Adjustments
- Adjustments made post-Cl2 etching indicated a need to evaluate wafer loading temperatures and quartz temperature differences post-processing. Key observations included potential necessity for tuning based on lower quartz temperatures observed.
Overall Performance & Future Considerations
Future analysis necessitates ongoing assessments of material stability and process efficiency as new methods are integrated into production.
The success criteria for upcoming tests includes stability attributes across thickness means and concentrations from the previous methodologies.
Continuing detailed inspections are essential for ensuring long-term stability and minimal degradation during chemical processes.