Comprehensive Study Guide to Metals, Nonmetals, Alloys, and Extraction Processes

Project and Research

  • Students are assigned to read from a reliable source concerning the uses of common metals and their compounds, specifically:
    • Sodium (NaNa)
    • Potassium (KK)
    • Magnesium (MgMg)
    • Calcium (CaCa)
    • Tantalum (TaTa)
  • Research findings are to be submitted to the teacher and discussed in class.

Alloys and Their Properties

  • Definition of Alloys: Alloys are mixtures of two or more metals, or metals combined with nonmetals. These constituents are melted together when molten and then allowed to cool to form a solid material. The constituent elements do not separate upon solidification.
  • Structural Difference (Figure 5.3):
    • Pure Metal: Atoms are of uniform size. Layers of atoms can easily slide over one another when a force is applied.
    • Alloy: The introduction of a second element with different-sized atoms stops the layers from sliding. This structural disruption makes sliding difficult, thereby increasing hardness and strength.
  • Effects of Alloying:
    • Increases hardness and strength.
    • Modifies the color and melting point.
    • Decreases electrical conductivity.
    • Increases resistance to corrosion.
  • Examples of Alloys:
    • Amalgam: An alloy of mercury (HgHg) combined with another metal.
    • Gun metal: Composed of copper (87 %87 \, \%), tin (10 %10 \, \%), and zinc (3 %3 \, \%).
    • Solder (Fuse Metal):
    • Composition: 67 %67 \, \% tin and 33 %33 \, \% lead.
    • Properties: Melts at 183 ∘C183 \, ^\circ\text{C}. This is significantly lower than the melting point of pure tin (232 ∘C232 \, ^\circ\text{C}).
    • Usage: Used to join wires and electrical resistances.

Gold Alloys and Content Measurement

  • Hardening Gold: Pure gold is very soft. It is hardened by alloying it with copper (CuCu) and silver (AgAg).
  • Gold Content (Carats): The quantity of gold in an alloy is expressed in carats or as a mass percent.
  • Carat Definition: A carat is equal to the mass unit of gold in 24 mass units24 \, \text{mass units} of the alloy.
    • 24 carat24 \, \text{carat}: Represents pure gold with no other metals.
    • 22 carat22 \, \text{carat}: Contains 22 parts22 \, \text{parts} of pure gold by mass in 24 parts24 \, \text{parts} of the alloy (commonly used for jewelry).
    • 18 carat18 \, \text{carat}: Contains 18 parts18 \, \text{parts} of pure gold by mass in 24 parts24 \, \text{parts} of the alloy.
  • Calculation of Mass Percent of Gold:
    • 24 Carat: Mass %=2424×100=100.00 %\text{Mass } \% = \frac{24}{24} \times 100 = 100.00 \, \% (Pure gold).
    • 22 Carat: Mass %=2224×100=91.67 %\text{Mass } \% = \frac{22}{24} \times 100 = 91.67 \, \% (Alloy containing 8.33 %8.33 \, \% CuCu or AgAg).
    • 18 Carat: Mass %=1824×100=75 %\text{Mass } \% = \frac{18}{24} \times 100 = 75 \, \%.

Production of Aluminum

  • Abundance and Importance:
    • Aluminum is the most abundant metal in the Earth's crust (8 %8 \, \% by mass).
    • It is the third most abundant element overall after oxygen and silicon.
    • In consumption, it ranks second globally after iron.
  • Natural Occurrence: Aluminum does not occur in a free metal state. Its main minerals include:
    • Bauxite (Al2O3⋅2H2OAl_2O_3 \cdot 2H_2O)
    • Cryolite (Na3AlF6Na_3AlF_6)
    • Corundum (Al2O3Al_2O_3)
    • Beryl (Be3Al2Si6O18Be_3Al_2Si_6O_{18})
    • China Clay (Al2Si2O5(OH)4Al_2Si_2O_5(OH)_4 or Al2Si2O8⋅2H2OAl_2Si_2O_8 \cdot 2H_2O)
The Hall-Héroult Process (Extraction of Aluminum)

Aluminum is extracted industrially from bauxite using the Hall-Héroult process.

  1. Purification of Bauxite:
    • Bauxite is often contaminated with silicon dioxide (SiO2SiO_2), iron oxide (Fe2O3Fe_2O_3), and titanium (IV) oxide (TiO2TiO_2).
    • The powdered ore is heated with an aqueous sodium hydroxide (NaOHNaOH) solution.
    • Silica conversion: SiO2(s)+2NaOH(aq)→Na2SiO3(aq)+H2O(l)SiO_2(s) + 2NaOH(aq) \rightarrow Na_2SiO_3(aq) + H_2O(l) (Soluble sodium silicate).
    • Aluminum oxide conversion: Al2O3(s)+2NaOH(aq)→2NaAlO2(aq)+H2O(l)Al_2O_3(s) + 2NaOH(aq) \rightarrow 2NaAlO_2(aq) + H_2O(l) (Soluble sodium aluminate).
    • Impurities: Iron oxides and titanium (IV) oxide are unaffected by the base and are removed via filtration.
  2. Precipitation and Calcination:
    • The solution is treated with acid: AlO2−(aq)+H3O+(aq)→Al(OH)3(s)\text{AlO}_2^-(aq) + H_3O^+(aq) \rightarrow Al(OH)_3(s).
    • Aluminum hydroxide is filtered, washed, dried, and heated strongly in a furnace (calcination):       2Al(OH)3(s)→HeatAl2O3(s)+3H2O(g)2Al(OH)_3(s) \xrightarrow{\text{Heat}} Al_2O_3(s) + 3H_2O(g)
  3. Electrolysis (Figure 5.4):
    • Pure Al2O3Al_2O_3 (alumina) is mixed with cryolite (Na3AlF6Na_3AlF_6) and fluorspar.
    • Role of Cryolite: Reduces the melting point of alumina from 2045 ∘C2045 \, ^\circ\text{C} to approximately 1000 ∘C1000 \, ^\circ\text{C} and provides a good conducting medium.
    • The Cell: A steel tank with a graphite (carbon) lining serving as the cathode. Graphite rods serve as the anode.
    • Electrode Reactions:
      • Anode (Oxidation): 3C(s)+6O2−(l)→3CO2(g)+12e−3C(s) + 6O^{2-}(l) \rightarrow 3CO_2(g) + 12e^- (The graphite anodes gradually oxidize and must be replaced regularly).
      • Cathode (Reduction): 4Al3+(l)+12e−→4Al(l)4Al^{3+}(l) + 12e^- \rightarrow 4Al(l).
      • Overall Reaction: 2Al2O3(l)+3C(s)→4Al(l)+3CO2(g)2Al_2O_3(l) + 3C(s) \rightarrow 4Al(l) + 3CO_2(g).
    • Molten aluminum is siphoned from the bottom of the cell.

Properties and Reactions of Aluminum

  • Physical Properties:
    • Soft, silvery-white, and lightweight.
    • Density: 2.7 g/cm32.7 \, g/cm^3.
    • Melting Point: 660 ∘C660 \, ^\circ\text{C}.
    • Highly ductile and malleable (wires, rolls, casts).
    • Excellent conductor of heat and electricity.
  • Chemical Properties:
    • Reaction with Oxygen: Forms a thin, protective film of aluminum oxide (Al2O3Al_2O_3) that inhibits further corrosion: 4Al(s)+3O2(g)→2Al2O3(s)4Al(s) + 3O_2(g) \rightarrow 2Al_2O_3(s).
    • Reaction with Nitrogen: Burns to form aluminum nitride: 2Al(s)+N2(g)→2AlN(s)2Al(s) + N_2(g) \rightarrow 2AlN(s).
    • Reaction with Acids: Reacts with dilute HClHCl and H2SO4H_2SO_4 to liberate hydrogen gas:
    • 2Al(s)+3H2SO4(aq)→Al2(SO4)3(aq)+3H2(g)2Al(s) + 3H_2SO_4(aq) \rightarrow Al_2(SO_4)_3(aq) + 3H_2(g)
    • 2Al(s)+6HCl(aq)→2AlCl3(s)+3H2(g)2Al(s) + 6HCl(aq) \rightarrow 2AlCl_3(s) + 3H_2(g)
    • Nitric Acid Exception: Does not react with dilute or concentrated HNO3HNO_3 due to the formation of a protective oxide layer. Thus, aluminum containers can transport HNO3HNO_3.
    • Reaction with Halogens: Burns in chlorine gas: 2Al(s)+3Cl2(g)→2AlCl3(s)2Al(s) + 3Cl_2(g) \rightarrow 2AlCl_3(s).
    • Reaction with Bases: Reacts with sodium hydroxide: 2Al(s)+2NaOH(aq)+6H2O(l)→2NaAl(OH)4(aq)+3H2(g)2Al(s) + 2NaOH(aq) + 6H_2O(l) \rightarrow 2NaAl(OH)_4(aq) + 3H_2(g).

Applications of Aluminum and Thermite Welding

  • General Uses: Duralumin alloys (Al, Cu, Mg) for aircraft, ships, and automobiles; household cookware (high thermal conductivity); window frames; roofing; food packaging; power transmission lines.
  • Thermite Welding:
    • Used for welding rails, propeller shafts, and heavy machinery parts.
    • The Process: Powdered aluminum mixed with iron (III) oxide (Fe2O3Fe_2O_3) is ignited, reaching temperatures of 3000 ∘C3000 \, ^\circ\text{C}.
    • Equation: 2Al(s)+Fe2O3(s)→2Fe(l)+Al2O3(s)2Al(s) + Fe_2O_3(s) \rightarrow 2Fe(l) + Al_2O_3(s).
    • Thermite Mixture: The specific mixture of powdered AlAl and Fe2O3Fe_2O_3.
    • Other applications: Used to isolate other metals like chromium: 2Al(s)+Cr2O3(s)→2Cr(l)+Al2O3(s)2Al(s) + Cr_2O_3(s) \rightarrow 2Cr(l) + Al_2O_3(s).

Production of Iron in the Blast Furnace

  • Iron Ores:
    • Hematite (Fe2O3Fe_2O_3) - Chief ore.
    • Magnetite (Fe3O4Fe_3O_4).
    • Siderite (FeCO3FeCO_3).
    • Limonite (Fe2O3⋅H2OFe_2O_3 \cdot H_2O).
    • Iron Pyrites (FeS2FeS_2), known as "fool's gold."
  • Raw Materials for Extraction: Iron ore, coke (fuel and reducing agent), limestone (flux), and hot air.
  • Process (Figure 5.5):
    1. Oxidation of Coke: C(s)+O2(g)→CO2(g)+HeatC(s) + O_2(g) \rightarrow CO_2(g) + \text{Heat} (2000 ∘C2000 \, ^\circ\text{C} near the bottom).
    2. Reduction to Carbon Monoxide: CO2(g)+C(s)→2CO(g)CO_2(g) + C(s) \rightarrow 2CO(g).
    3. Reduction of Iron Oxides:
      • 3Fe2O3(s)+CO(g)→2Fe3O4(s)+CO2(g)3Fe_2O_3(s) + CO(g) \rightarrow 2Fe_3O_4(s) + CO_2(g)
      • Fe3O4(s)+CO(g)→3FeO(s)+CO2(g)Fe_3O_4(s) + CO(g) \rightarrow 3FeO(s) + CO_2(g)
      • FeO(s)+CO(g)→Fe(l)+CO2(g)FeO(s) + CO(g) \rightarrow Fe(l) + CO_2(g)
    4. Limestone Decomposition and Slag Formation:
      • Flux reaction: CaCO3(s)→CaO(s)+CO2(g)CaCO_3(s) \rightarrow CaO(s) + CO_2(g).
      • Scavenging silica (sand) impurity: CaO(s)+SiO2(s)→CaSiO3(l)CaO(s) + SiO_2(s) \rightarrow CaSiO_3(l).
      • Slag: Molten calcium silicate is lighter than molten iron and floats on top. It is used in cement manufacturing.

Types of Iron and Steel Making

  • Pig Iron (Crude Iron): Obtained directly from the blast furnace. Contains 92 %92 \, \% iron, 3.5–4.5 %3.5 \text{--} 4.5 \, \% carbon, and smaller amounts of silicon (2 %2 \, \%), phosphorus (1 %1 \, \%), manganese, and sulfur. It is very brittle.
  • Cast Iron: Formed by re-melting pig iron with scrap iron and casting into molds.
  • Wrought Iron: The purest commercial form (99.5 %99.5 \, \% iron). Tough, malleable, and ductile. Made by heating impure iron with hematite and limestone.
  • Steel Making (Purification): The process of removing excess carbon and impurities through oxidation at high temperatures.
  • Techniques:
    1. Bessemer Converter: Molten pig iron is placed in a vessel with a magnesium and calcium carbonate lining. Hot air is blown through holes in the bottom. Takes only 15 minutes15 \, \text{minutes} but quality is variable and difficult to control.
    2. Open-hearth Furnace: Large shallow hearth lined with MgOMgO and CaOCaO. Charged with pig iron, Fe2O3Fe_2O_3, scrap iron, and limestone. Impurities like carbon and sulfur bubble out as gases (CO2CO_2, SO2SO_2). Takes 8–10 hours8 \text{--} 10 \, \text{hours}; quality is better controlled.
    3. Basic Oxygen Process: Powdered CaOCaO and oxygen gas are forced onto the surface of molten pig iron via an oxygen lance. Highly exothermic. Takes 20–25 minutes20 \text{--} 25 \, \text{minutes}. This has largely replaced the open-hearth method.
  • Tempering: A process of heating and controlled cooling to achieve desired hardness. Removes cementite (Fe3CFe_3C), which otherwise reduces steel hardness.

Physical and Chemical Properties of Iron

  • Physical Properties:
    • Gray, lustrous, malleable, and ductile.
    • Density: 7.87 g/cm37.87 \, g/cm^3.
    • Melting Point: 1580 ∘C1580 \, ^\circ\text{C}.
    • Ferromagnetic: Can be permanently magnetized.
  • Chemical Properties:
    • Rusting: Occurs in the presence of air and moisture, forming hydrated iron (III) oxide (Fe2O3⋅xH2OFe_2O_3 \cdot xH_2O).
    • Reaction with Acids: Forms iron (II) salts and H2H_2: Fe(s)+2HCl(aq)→FeCl2(aq)+H2(g)Fe(s) + 2HCl(aq) \rightarrow FeCl_2(aq) + H_2(g).
    • Oxidation States: Common states are Fe2+Fe^{2+} (ferrous - pale green) and Fe3+Fe^{3+} (ferric - yellowish brown).
    • Oxidation of Hydroxides: 4Fe(OH)2(s)+O2(g)+2H2O(l)→4Fe(OH)3(s)4Fe(OH)_2(s) + O_2(g) + 2H_2O(l) \rightarrow 4Fe(OH)_3(s).
    • Reaction with Halogens/Sulfur:
    • 2Fe(s)+3Cl2(g)→2FeCl3(s)2Fe(s) + 3Cl_2(g) \rightarrow 2FeCl_3(s)
    • Fe(s)+S(s)→FeS(s)Fe(s) + S(s) \rightarrow FeS(s)
    • Displacement Reactions: Iron displaces less active metals like copper from solutions: Fe(s)+Cu2+(aq)→Fe2+(aq)+Cu(s)Fe(s) + Cu^{2+}(aq) \rightarrow Fe^{2+}(aq) + Cu(s).

Classification of Steels

Type% CarbonTypical Uses
Mild SteelUp to 0.2 %0.2 \, \%Screws, motors, railway lines, ships, nuts, bolts
Medium Steel0.3–0.6 %0.3 \text{--} 0.6 \, \%Springs and chains
High Carbon Steel0.6–1.5 %0.6 \text{--} 1.5 \, \%Drill bits, knives, hammers, chisels
Stainless Steel1 % C,18 % Cr,8 % Ni1 \, \% \, C, 18 \, \% \, Cr, 8 \, \% \, NiKitchen pots, pans, food machinery, laundry machines
  • Alloy Steel: Contains higher percentages of other metals (Chromium, Nickel, Tungsten, Manganese) to provide hardness, toughness, and heat resistance.

Occurrence and Extraction of Copper

  • Minerals:
    • Sulphide ores: Chalcopyrite (CuFeS2CuFeS_2), Chalcocite (Cu2SCu_2S), Covellite (CuSCuS), Bornite (Cu5FeS4Cu_5FeS_4).
    • Oxide ores: Cuprite (Cu2OCu_2O), Tenorite (CuOCuO).
    • Carbonate ores: Malachite (CuCO3⋅Cu(OH)2CuCO_3 \cdot Cu(OH)_2).
  • Extraction Process (from Chalcopyrite):
    1. Concentration: Crushed ore is concentrated by froth flotation, increasing copper content from 2 %2 \, \% to 30 %30 \, \%.
    2. Roasting: 2CuFeS2(s)+4O2(g)→Cu2S(s)+2FeO(s)+3SO2(g)2CuFeS_2(s) + 4O_2(g) \rightarrow Cu_2S(s) + 2FeO(s) + 3SO_2(g).
    3. Smelting: Limestone and sand (SiO2SiO_2) are added to remove iron oxide and silica as slag:
      • FeO(s)+SiO2(s)→FeSiO3(l)FeO(s) + SiO_2(s) \rightarrow FeSiO_3(l)
      • CaCO3(s)+SiO2(s)→CaSiO3(l)+CO2(g)CaCO_3(s) + SiO_2(s) \rightarrow CaSiO_3(l) + CO_2(g)
    4. Reduction: The obtained Cu2SCu_2S is heated with a limited oxygen supply to produce copper: Cu2S(s)+O2(g)→2Cu(l)+SO2(g)Cu_2S(s) + O_2(g) \rightarrow 2Cu(l) + SO_2(g).

Questions & Discussion

Activity 5.2 (Aluminum)

  1. Question: What properties of aluminum make it useful for packaging cigarettes and medicines?
    • Response: Malleability (can be rolled into thin foil) and resistance to corrosion.
  2. Question: Why are steel-cored aluminum cables used for high-voltage electricity?
    • Response: Aluminum is a good conductor and lightweight; the steel core provides structural strength to prevent the cable from sagging or breaking over long distances.
  3. Question: Materials in your home made of aluminum?
    • Response: Cans, foil, pots, window frames; noted for light weight, lack of rusting, and ease of shaping.

Activity 5.3 (Aluminum Reactivity/Cooking)

  1. Question: Why should food containing iron salts not be cooked in aluminum utensils?
    • Response: Due to displacement reactions where the more reactive aluminum might displace iron.
  2. Question: Aluminum is highly reactive, yet used for utensils. Why?
    • Response: The instantaneous formation of a thin, protective layer of Al2O3Al_2O_3 prevents further reaction with food or water.

Activity 5.5 (Blast Furnace)

  1. Question: Explain the principle of the blast furnace.
    • Response: It uses counter-current reduction where rising COCO gas reduces descending iron ore while limestone removes impurities as slag.
  2. Question: Why is calcium carbonate used?
    • Response: To act as a flux that reacts with acidic impurities (like sand) to form slag.

Activity 5.6 (Iron/Steel)

  1. Question: Which form of iron is the purest?
    • Response: Wrought iron (99.5 %99.5 \, \% iron).