Overview of Steel and Iron Production
- Steel vs. Iron
- The advantage of steel over pure iron lies in its superior strength.
- Steel is defined as iron with small amounts of carbon, typically around 2%.
Iron Ore Composition
- Types of Iron Ore
- The primary components of iron ore are iron oxides:
- Hematite: Fe2O3
- Magnetite: Fe3O4 - Forms of Iron Ore:
- Iron ore can exist in several forms, each with varying size:
- Lumps: Approximately 22 mm in size
- Pellets: Approximately 12 mm in size
- Fines: Approximately 5 mm in size - Iron Product Forms:
- Iron products are produced in the form of pellets, lumps, or briquettes.
Preparation of Iron Ore
- Storage and Handling
- Crushed iron ore is received from ships and stored in large stockpiles.
- The stored ore is screened and then housed in large containers known as 'day bins'.
- The oxide handling system delivers raw material to the furnace charge hopper using conveyor systems.
- The hopper is integral to the oxide feed system, distributing the material evenly and maintaining a continuous oxide supply to the furnace. - Distribution Importance
- It is essential for solids to be distributed in a symmetrical pattern about the charge hopper center-line to ensure proper function.
- The oxide feed system additionally serves as a dynamic gas seal leg, preventing gas from escaping the furnace to the atmosphere.
Reduction Process
- Fundamentals of Reduction
- The core task of the reduction process is to remove oxygen from the iron ore.
- Reducing gas, which is a mixture of hydrogen and carbon monoxide, acts as the reducing agent.
- The chemical interaction results in the formation of iron, carbon dioxide, and water vapor. - Chemical Reactions
- The primary reactions are:
- Fe_2O_3 + 3H_2
ightarrow 2Fe + 3H_2O
- Fe_2O_3 + 3CO
ightarrow 2Fe + 3CO_2 - Gas Quality
- The effectiveness of the reducing gas is contingent upon the ratio of reducing gases to oxidizing agents (such as CO2 and H2O(g)) in the mixture, referred to as gas quality.
- A requisite gas quality range of 10-12:1 is essential for fresh hot reducing gas.
- Higher gas quality leads to a lower volume of gas required for reactions, enhancing process efficiency.
- For complete reaction, the flow of reducing gas per unit mass of iron must ensure that the gas quality leaving the furnace is at least 2:1.
- Catalytic Reforming
- The process involves the catalytic reforming of natural gas with steam in a reactor, utilizing either nickel or cobalt catalysts at temperatures between 900-1000°C.
- This reforming takes place in catalyst-filled tubes that are heated inside a refractory-lined furnace (known as a reformer). - Gas Processing
- The top gas, derived from furnace off-gas and recycled, is compressed and mixed with natural gas before entering the reformer tubes.
- Waste CO2 from the furnace reacts with natural gas, contributing to the production of additional reformed gas. - Chemical Reactions in Reforming
- The chemical equations governing the reforming reactions are:
- CH_4 + H_2O
ightarrow CO + 3H_2
- CH_4 + CO_2
ightarrow 2CO + 2H_2
Carburization Process
- Objective and Method
- The aim of the carburization process is to augment the carbon content within metallic iron.
- Natural gas is introduced into the furnace to facilitate this increase in carbon content. - Chemical Reactions in Carburization
- The following chemical equations describe the carburization interactions:
- 3Fe + CH_4
ightarrow Fe_3C + 2H_2
- 3Fe + 2CO
ightarrow Fe_3C + CO_2
Visual Flow Diagram
- Components and Flow
- Iron ore, steam, top gas, recycle gas, scrubber, reducing gas, natural gas, and product flow structures are vital to the functioning of the entire process.
References
- The MIDREX Process brochure (online)
- Arcelor Mittal Steel Company