BIOP 5250


EXAM 1 QUESTIONS


Which is most likely the correct order to increase tensile strength?

  • Cellulose>Hemicellulose>Lignin

pMDI is more costly than PF


IMPORTANT CONCEPTS

  1. 4 general composite types:

  • PLYWOOD

    • veneers are laid CROSSWAYS

      • WHY?

        • improves dimensional stability

        • stabilizes strength in the perpendicular direction due to grain direction in core\

        • stiff material can be placed on the faces

  • ORIENTED STRAND BOARD

  • PARTICLEBOARD

  • FIBERBOARD


  1. Adhesive curing process in composites

  •  apply heat + pressure → viscosity initially decreases (thermoplastic-like flow) —> viscosity then increases due to polymerization/cross-linking → duration of the thermoplastic (flowable) phase controls how well the resin penetrates the wood → resin becomes semi-solid to solid (50-100% cure) → PF resin, in particular, can continue curing during hot-stacking after pressing

  1. Aspect ratio is fiber length/fiber diameter

  2. BIOCOMPOSITE

  • definition: a material formed by a matrix (resin) and a reinforcement of natural fibers, usually derived from plants or cellulose

  • can be treated as laminates — each layer engineered with a specific mechanical/physical property to yield a desired macro (whole composite) response

  • Most biocomposites are anisotropic (directional properties)

  1. cellulose, hemicellulose, lignin degradation temperature

  • hemicellulose degrades at the lowest temperature

    • followed by cellulose

    • LIGNIN degrades across the broadest and highest temperature range

  1. Cellulose, hemicellulose, hemicellulose - structure/role/strength ranking


cellulose

highest stiffness, linear, higher modulus (134 GPas) highly crystalline polysaccharide

acts as the reinforcing “rod” in wood’s natural composite structure

Hemicellulose

much lower in strength than cellulose, branched, lower-molecular-weight polysaccharide with a very low modulus (0.04 GPas) when moist

chemically bridges cellulose and lignin (they have no natural affinity for each other) so stress can transfer to the cellulose

Lignin

generally the weakest in tension, rigid, phenolic (non-carbohydrate) polymer that acts more as a binding/encrusting agent, gluing cells together and adding compressive rigidity and dimensional stability rather than tensile strength

  1. Composite (engineering definition): a material made from two or more constituent materials with significantly physical or chemical properties, which remain separate and distinct on a macroscopic level within the finished structure

  2. Composite density: generally increases with reduction in particle size

  3. Concentrated Static Load: sample 10 boards; if 100% exceed the load threshold → pass

  • if one board fails, test 10 more.

  • PS2 calls this a “95% passing rate,” but because companies target the mean at 95% pass, real-world compliance often lands closer to about 80% actual pass rate”

  1. Conformability: the ability of paper to bend, flex, and conform to the shape of a container or mold without tearing or losing structural integrity.

  • important for molded fiber packaging (trays, clamshells) and for developing good hydrogen bonding between fibers (fibers need to conform to make close contact)

  1. Continuous vs. Discontinuous fibers

  • continuous - very long; provides an unbroken load path through the composite

  • discontinuous - chopped/short sections (L/D roughly <100)

  1. Creep (primary/secondary/tertiary)

primary (transient) creep - strain rate is a function of time (decreasing rate)

secondary (steady-state) creep - dislocation structure/grain size reach equilibrium; strain rate is roughly constant

tertiary creep - strain rate increases exponentially with stress (leads toward failure)

Creep depends on the amorphous vs crystalline ratio of the polymer/cellulose in the composite

→ more crystalline cellulose = more elastic, less creep

Maxwell vs Kelvin-Voigt

→ Maxwell model: spring and dashpot in series

  • more viscous

→ Kelvin-Voigt: spring and dashpot in parallel

  • more elastic

  1. Paper cross direction vs Machine direction

  • Machine direction: direction the sheet travels through the paper machine — fibers tend to align this way, giving higher strength/stiffness along MD

  • Cross direction: perpendicular to machine direction — generally lower strength, higher stretch than MD

  1. Equilibrium Moisture Content

  • the moisture content at which wood/fiber material neither gains nor loses moisture to the surrounding environment — governed by relative humidity

13. Factors contribute to Bond Formation in Wood

  • Anatomical section: radial, tangential, or transverse

  • Density / porosity; earlywood (springwood) vs latewood (summerwood)

  • moisture content and its distribution - pMDI tolerates/loves water; PF does not tolerate it well

  • Extractives content

  • Heartwood vs sapwood

  • pH of the wood

  • Fiber surface quality (smooth vs. rough) and any surface treatment

  • Temperature of the fiber/element at bonding

  • Geometry of the element

  • Species/plant type (hardwood vs. softwood

  1. Fiber refining

  • increases bonded surface area between fibers (better inter-fiber bonding) but can introduce micro-compressions that weaken individual fibers

  1. Green composite - Bonded via natural mechanisms (e.g., hydrogen bonding between cellulose) with no synthetic adhesive — relevant to MDF, paper, WPC fiber-to-fiber bonding.

  2. MDI vs. PF - pMDI: pricier, no formaldehyde emission, better moisture resistance, needs a release agent (sticks to steel). PF: ~ half the cost, does emit formaldehyde, less moisture resistant, needs ~ 2x the loading for equal strength

  3. 3 bonding mechanisms

    1. Mechanical interlocking (physical intertwining, ~2-6 fibers deep),

    2. physical attraction (van der Waals/hydrogen bonding)

    3. covalent chemical bonding (true electron-sharing, e.g., pMDI’s - NCO + wood - OH → urethane linkage - the “holy grail,” still debated

  4. Paper moisture content - affects both strength and extensibility of the fiber network; tied closely to EMC and hysteresis (the wetting curve does not equal the drying curve at the same RH )

  5. Particle size effects - smaller particles → lower clear-wood strength (defects removed) but less property variation (average), and generally higher density

  6. Rule of mixtures - composite property = weighted average of constituent properties, weighted by volume/mass fraction

  7. “Nature’s way to engineer a fiber” - The wood cell wall’s layered cellulose/hemicellulose/lignin structure is naturally optimized composite, built to resist loads like wind on a standing tree

  8. Wood anatomy and chemistry - Density, earlywood/latewood, microfibril angle, and chemical composition all drive bonding behavior and mechanical performance of the resulting composite

  9. Wood cell wall structure - cellulose microfibrils embedded in a hemicellulose/lignin matrix; microfibril angle (MFA) strongly affects stiffness (lower MFA = generally stiffer)

  10. Wood composite processing flow - raw Material → sort and store → size reduction → screen → dry → blend → form (mat) → press → trim → sand → overlay → sales